Material Notes:
Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhibits good toughness, superior biaxial stretchability, and flexibility even at low temperatures. It is insensitive to stress cracking and notch effects. Special stabilization provides good resistance to heat ageing and UV radiation. Lucolit is thus to a large extent resistant to weathering and ageing.Applications:• Roofing sealing and membranes• Construction profiles and water stops• Injection molded parts in the building sectorInformation provided by Lucobit AG
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
ISO 1183
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ISO 868
Modulus of Elasticity 0.0800 GPa
11.6 ksi
ISO 527
Thermal Properties Metric English Comments
Minimum Service Temperature, Air <= -45.0 °C
<= -49.0 °F
Low Temperature Flexural Test; DIN 53361
Processing Properties Metric English Comments
Processing Temperature 150 - 200 °C
302 - 392 °F
Profiles
160 - 230 °C
320 - 446 °F
Membranes
160 - 270 °C
320 - 518 °F
Coatings
Melt Temperature 160 - 220 °C
320 - 428 °F
Mold Temperature 10.0 - 40.0 °C
50.0 - 104 °F
Copyright © lookpolymers.com All Rights Reserved