| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.980 g/cc | 0.0354 lb/in³ | |
|
Premix Thermoplastics PRE-ELEC® ESD 2300
PRE-ELEC ESD 2300 is a static dissipative thermoplastic compound based on PE-HD. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 2300 has been developed for mult..
|
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ISO 1183 |
|
Polykemi AB POLYelast TPE 10012 R3 Thermoplastic Elastomer, PP/Elastomer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | TPE-0105 (ASTM D792) |
|
Advanced Elastomer Systems Santoprene® 281-73 Thermoplastic Rubber
(discontinued **)
A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be ..
|
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ISO 2781 |
|
Termopol Termoton® V5GA1090A TPV Compound
Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;..
|
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ISO 1183 |
|
LATI LATISTAT 43/7-02 Low Density Polyethylene (LDPE) Base Conductive Plastic
(discontinued **)
Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable..
|
|||
| Density | 0.980 - 1.10 g/cc | 0.0354 - 0.0397 lb/in³ | Average value: 1.04 g/cc Grade Count:84 |
|
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..
|
|||
| Density |
0.980
g/cc <br>@Temperature 20.0 °C
|
0.0354
lb/in³ <br>@Temperature 68.0 °F
|
|
|
LyondellBasell DPMA Dipropylene glycol methyl ether acetate
Information provided by Lyondell.
|
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
|
Global CPP-110 10% CaC03 Filled Polypropylene
Information provided by Global Polymers Corporation.
|
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | Uncured |
|
ITW Plexus Plexusâ„¢ AO420FS Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.
|
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
|
Multibase Multi-Flex® TPE A 5402 BLK
The burn rate is 0.7 in/min based on ASTM FM VSS 302. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
|
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ISO 1183 |
|
LyondellBasell Hostacomâ„¢ CB275FC Thermoplastic Polyolefin Elastomer
Description: Hostacomâ„¢ CB275FC high melt flow, 1,900 MPa flexural modulus, precolored, UV-stabilized, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of pro..
|
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
|
Techmer ES HiFill® PP GF10 CC 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc.
|
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
|
Techmer ES HiFill FR® HDPE FR-2
Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc.
|
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
|
Techmer ES HiFill® LDPE 0098 S LE
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforAdditive: Heat StabilizerFeatures: Low ExtractablesInformation provided by TP Composites, Inc.
|
|||
| Density | 0.980 - 1.00 g/cc | 0.0354 - 0.0361 lb/in³ | |
|
Wacker Silicones Geniomer® 140 Silicone TPE
SLM TPSE 140 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas..
|
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
|
Tipco Tipcolene® FPC 10 - 10% Calcium Carbonate Reinforced Polypropylene Homopolymer
10% Calcium Carbonate Filled PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
|
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
|
Tipco Tipcolene® FPT 10 PPC - 10% Talc Reinforced Polypropylene Copolymer Compound
10% Talc Reinforced PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India.
|
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | |
|
Dow Corning SYL-OFF® PMCPSL 11 Crosslinker
This Syl-Off ® Crosslinker is one component of a multi-component silicone release coating system. In order to use this product effectively, it must be blended with the appropriate Syl-Off ® coatin..
|
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | Melt |
|
Covestro Desmopan® DP 9392AU Polyurethane
Extrusion- and injection molding gradewith special UV stabilizersvery good hydrolysis and microbial resistancegood low-temperature flexibilityApplicationHosesnon-reinforcedCable sheathingsProfilesTe..
|
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | |
|
DuPont™ Nomex® 414 Paper, 15 mil Nominal Thickness
Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand..
|
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
|
Entec Hypro™ PPH-T10 Homopolymer Polypropylene, 10% Talc Reinforced
Information provided by Entec
|
|||
| Density | 0.980 - 0.990 g/cc | 0.0354 - 0.0358 lb/in³ | |
|
BASF 3-Amino-1-propanol
Formula: C3H9NOCAS: 156-87-6Description: 3-amino-1-propanol is a colorless to yellow liquid with an amine-like odor. It is miscible with water in all proportions. Synonyms: Propanolamine, 3-aminopr..
|
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | |
|
3M 9082UV Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
|
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | |
|
BASF Procom® X10S 773 Polypropylene
Car bumpers and spoilers where good paintability is required.Data was collected by ISO methods and provided by BASF.
|
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
|
Multibase Multi-Flam™ 0106 PP Polypropylene
Features:Flame RetardantHalogenated Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureInformation provided by Multibase
|
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | |
|
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**)
Unreinforced Polyamide 66Zytel 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
|
|||
| Density |
0.980
-
0.980
g/cc <br>@Temperature 285 - 285 °C
|
0.0354
-
0.0354
lb/in³ <br>@Temperature 545 - 545 °F
|
Average value: 0.980 g/cc Grade Count:1 |
|
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..
|
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D 792 |
|
SABIC Innovative Plastics LNP Stat-kon MD000IU PP (Asia Pacific)
LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa..
|
|||