| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.980 g/cc | 0.0354 lb/in³ | STN EN ISO 1183-1 |
| Plastcom PLASTALEN® PC 69 T 10 003 Polypropylene reinforced with mineral filler Modified PP copolymer for injection molding with the content of 10% mineral filler. Application in all automotive industry. Delivered in black.Information Provided by Plastcom spol. s r.o. |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ISO 1183A |
| Mytex Polymers AS171L-02US Polypropylene, 13% Talc Filled AS171L-02US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability.This product is available .. |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ISO 1183 |
| Polyplastic Armlen® PP-2FR Polypropylene, Flame Retardant Flame retardant, RoHS compliantInformation provided by PolyPlastic Group. |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | |
| Premix Thermoplastics PRE-ELEC® PP 1399 Dissipative Thermoplastic Compound PRE-ELEC® PP 1399 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resi.. |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ISO 1183 |
| Polykemi AB POLYfill PP HJ752 Polypropylene/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ISO 2781 |
| Termopol Termoton® V5GA1090A TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ISO 1183 |
| LATI LATISTAT 43/7-02 Low Density Polyethylene (LDPE) Base Conductive Plastic
(discontinued **) Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable.. |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | TA4302B |
| Permabond TA4302 Toughened Acrylic Adhesive PERMABOND® TA4302 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni.. |
|||
| Density | 0.980 - 0.980 g/cc @Temperature 290 - 290 °C |
0.0354 - 0.0354 lb/in³ @Temperature 554 - 554 °F |
Average value: 0.980 g/cc Grade Count:1 |
| Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
| SABIC Innovative Plastics LNP STAT-KON MX10301C PP LNP* STAT-KON* MX10301C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System. |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | |
| Stellarchem SE/PA745B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
| Techmer ES HiFill® PP GF10 CC 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | |
| Silon PA 0835 HD Processing Aid Concentrate Masterbatch with a highly effective processing aid for polyethylene, especially PE-HD. By using the PA 0835 HD, the output can be markedly increased and the pressure build-up in the barrel decreased.. |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | |
| Solvay ALKAMULS® S 90 Surfactant Identification: SORBITAN MONOISOSTEARATECAS: 71902 – 01 – 7EINECS: 276 – 171 – 2Available in: Asia Pacific, Europe, Latin America and North America.Applications: Water/Oil emuls.. |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ISO 1183 |
| Borealis Daplen™ EH104AE Polypropylene TPO Compound Daplen™ EH104AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, high.. |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
| Tipco Tipcolene® FPC 10 PPC - 10% Calcium Carbonate Reinforced Polypropylene Copolymer 10% Calcium Carbonate Filled PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India. |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
| Tipco Tipcolene® FPT 10 - 10% Talc Reinforced Polypropylene Homopolymer 10% Talc Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ISO 1183 |
| Tisan TISOPLEN® 10% Calcite Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
| Plastics Group Polifil® GFRMPPCC-10 10% Glass Reinforced Polypropylene, High Impact Polifil® GFRMPPCC series compounds are high impact polypropylenes reinforced with chemically coupled glass fibers. This combination provides higher impact strength while retaining high stiffness.Ap.. |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | |
| Dow Corning SYL-OFF® PMCPSL 1 Crosslinker Information provided by Dow Corning |
|||
| Density | 0.980 g/cc @Temperature 330 °C |
0.0354 lb/in³ @Temperature 626 °F |
Melt |
| Covestro Apec® 1800 Polycarbonate Basic gradesoftening temperature (VST/B 120)=185 °CPreprocessingMax. Water content |
|||
| Density | 0.980 g/cc @Temperature 330 °C |
0.0354 lb/in³ @Temperature 626 °F |
Melt |
| Covestro Apec® 1803 Polycarbonate UV-stabilizedsoftening temperature (VST/B 120)=184 °CPreprocessingMax. Water content |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | Melt |
| Covestro Desmopan® 9385 Polyurethane Extrusion- and injection molding gradevery good hydrolysis and microbial resistancegood low-temperature flexibilitycomplies with VDE 0282-10ApplicationCable sheathingsHosesnon-reinforcedPreprocessin.. |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
| Entec Hypro™ PPC-GF10 Natural Impact Polypropylene, 10% Glass Reinforced Information provided by Entec |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D297 |
| Dow Nordel® NDR 47100.00 EPDM Hydrocarbon Rubber Description: NDR 47100 is a developmental product in granular form that contains carbon black as a partitioning agent. It is a high molecular weight semi-crystalline EPDM grade with high green stren.. |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | |
| 3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ASTM D792 |
| Multibase Multi-Flam™ 0106 PP Polypropylene Features:Flame RetardantHalogenated Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureInformation provided by Multibase |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | |
| DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
| Density | 0.980 g/cc | 0.0354 lb/in³ | ISO 1183 |
| Lucobit Lucolit® 1320 Polyolefin TPO Granules, Beige Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi.. |
|||