Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Processing Temperature = 446 °F Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
ExxonMobil Santoprene® 8123-45S100 Thermoplastic Elastomer  (discontinued **)
A hard, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has low friction and is especially designed for use as a co-extruded slip-coat layer on weath..
Processing Temperature 175 - 230 °C
347 - 446 °F
ExxonMobil Vyram™ 9101-45 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
Processing Temperature 175 - 230 °C
347 - 446 °F
ExxonMobil Vyram™ 9111-35W222 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for use in difficult injection molding applications and those requiring good flex..
Processing Temperature 190 - 230 °C
374 - 446 °F
PolyChem Alloy PolyFoam 4006F
PolyFoam decomposes when heated to create a uniform microcellular structure. It can be used in extrusion and injection molding processes to reduce weight in parts without adversely affecting the ph..
Processing Temperature 177 - 230 °C
350 - 446 °F
Average value: 199 °C Grade Count:29
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
Processing Temperature 210 - 230 °C
410 - 446 °F
Taiwan Sheen Soon Sheenthane® D7620 Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
Processing Temperature 220 - 230 °C
428 - 446 °F
C2
UBE 5033B Air Blown Nylon 6/66 Film
Specialties: Standard nylon 6/66Medium shrink, Low slipApplications: Best for Middle layer usageProcessing: Top web (Air blown)Thermoforming (T-die)Information provided by UBE.
Processing Temperature 170 - 230 °C
338 - 446 °F
Zhejiang Juner PP6-1JE PP For Automotive Parts
Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd.
Processing Temperature 180 - 230 °C
356 - 446 °F
Blow Molding
Total Lumicene® mPE M 2310 EP Metallocene Polyethylene, Blown Film
Lumicene® mPE M 2310 EP is a second generation metallocene based Linear Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2310 EP can be processed at high output rates with low ext..
Processing Temperature 175 - 230 °C
347 - 446 °F
ExxonMobil Santoprene® 103-40 Thermoplastic Elastomer
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Processing Temperature 175 - 230 °C
347 - 446 °F
ExxonMobil Santoprene® 121-58W175 Thermoplastic Elastomer
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for ..
Processing Temperature 175 - 230 °C
347 - 446 °F
ExxonMobil Santoprene® 121-70B230 Thermoplastic Elastomer
A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated to bond to sulfur or peroxide-cured thermoset EPDM rubber for corner ..
Processing Temperature 175 - 230 °C
347 - 446 °F
ExxonMobil Santoprene® 123-50W175 Thermoplastic Elastomer
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in thin wall ..
Processing Temperature 175 - 230 °C
347 - 446 °F
ExxonMobil Santoprene® 8221-70 Thermoplastic Elastomer
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
Processing Temperature 180 - 230 °C
356 - 446 °F
Barrel temperature
Azoty Tarnow™ TARNOFORM 300 GF7 POM
35% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A...
Processing Temperature 180 - 230 °C
356 - 446 °F
Barrel temperature
Azoty Tarnow™ TARNOFORM 300 SI POM
Tribological modified grade with silicon, for better sliding properties in plastic-plastic contact.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Processing Temperature 190 - 230 °C
374 - 446 °F
Injection
Alliance Polymers Viprene™ G70A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G70A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Processing Temperature 200 - 230 °C
392 - 446 °F
Injection
Alliance Polymers Viprene™ P90A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P90A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Processing Temperature 180 - 230 °C
356 - 446 °F
Resin Temp.
Beijing Chemical Industry KAIFA® GL5200 ABS Extrusion Grade
Non-toxic, Superior impact strength at low temp., High gloss, Uniform sheet thickness for vacuum moldingInformation provided by Beijing Chemical Industry Research Institute (Group)
Processing Temperature 175 - 230 °C
347 - 446 °F
ExxonMobil Santoprene® 171-55 Thermoplastic Elastomer  (discontinued **)
A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those..
Processing Temperature 175 - 230 °C
347 - 446 °F
ExxonMobil Vyram™ 9201-55 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..
Processing Temperature 160 - 230 °C
320 - 446 °F
Flat-sheet
Lucobit Lucofin® 1400HN Ethylene Butyl Acrylate
Lucofin 1400HN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN is softer and more flexible than ethylene homopolym..
Processing Temperature 160 - 230 °C
320 - 446 °F
Membranes
Lucobit Lucolit® 1310 Polyolefin TPO Granules, Grey
Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi..
Processing Temperature 175 - 230 °C
347 - 446 °F
ExxonMobil Santoprene® 8211-60 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, non-hygroscopic, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance ..
Processing Temperature 175 - 230 °C
347 - 446 °F
ExxonMobil Santoprene® 111-87 Thermoplastic Elastomer  (discontinued **)
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Processing Temperature 185 - 230 °C
365 - 446 °F
Metering Zone
Wacker Silicones Geniomer® 60 Silicone TPE
SLM TPSE 60 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase..
Processing Temperature 175 - 230 °C
347 - 446 °F
ExxonMobil Santoprene® 221-80 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
Processing Temperature 175 - 230 °C
347 - 446 °F
ExxonMobil Santoprene® 221-87W211 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
Copyright © lookpolymers.com All Rights Reserved