Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
Water Absorption | 0.30 % | 0.30 % | ISO 62 |
Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | |
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | ISO 1133 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell M | 98 | 98 | ISO 2039-2 |
Ball Indentation Hardness | 185 MPa | 26800 psi | ISO 2039-1 (H 961-30) |
Tensile Strength | 83.0 MPa | 12000 psi | ISO 527 |
Elongation at Break | 5.0 % | 5.0 % | ISO 527 |
Flexural Strength | 115 MPa | 16700 psi | ISO 178 |
Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178 |
Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | ISO 180/1A |
Charpy Impact Unnotched | 2.00 J/cm² | 9.52 ft-lb/in² | ISO 179/1eU |
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | ISO 179/1eA |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ISO 75B |
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | ISO 75A |
Vicat Softening Point | 109 °C | 228 °F | ISO 306B |
117 °C | 243 °F | ISO 306A | |
Flammability, UL94 | HB | HB | |
Glow Wire Test | 650 °C | 1200 °F | IEC 695-2-1 |
Optical Properties | Metric | English | Comments |
---|---|---|---|
Refractive Index | 1.49 | 1.49 | ISO 489 |
Haze | 0.40 % | 0.40 % | ASTM D1003 |
Transmission, Visible | 92 % | 92 % | ASTM D1003 |