Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 216 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
<br>@Thickness 3.20 mm
216 °F
<br>@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Asia Pacific)
High impact PC+ABS material designed for local Pacific Automotive applications
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
216 °F
ASTM D648
Gichem GILAC A070V3C Acrylonitrile Butadiene Styrene &nbsp;(discontinued **)
ABS glass fiber filled, excellent mechanical properties. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
216 °F
ASTM D648
LG Chemical HP PMMA
Information Provided by LG Chem
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
<br>@Thickness 6.40 mm
216 °F
<br>@Thickness 0.252 in
Unannealed; ASTM D648
LG Chemical LUPOS GP2206F ABS+GF20%, Flame Retardant
Feature: Injection Molding, ABS+GF20%, Flame RetardantApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7, 65997-17-3, 88497-56-7 and 1309-64-4Information provided b..
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
<br>@Thickness 6.40 mm
216 °F
<br>@Thickness 0.252 in
ASTM-D648
Ineos ABS Lustran® ABS 241 ABS, Blending Grade
Lustran® ABS 241 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v..
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
216 °F
ISO 75A
Lucite International Diakon® CMG334V Acrylic Polymer
Information provided by Lucite International
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
216 °F
ISO 75A
Lucite International Diakon® CMH454L Acrylic Polymer
Information provided by Lucite International
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
216 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP LUBRICOMP OL004 PPS - Linear
LNP* LUBRICOMP* OL004 is a compound based on PPS - Linear resin containing 20% PTFE. Added features of this grade include: Wear Resistant.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
216 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER
PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
<br>@Thickness 3.20 mm
216 °F
<br>@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics LNP Thermocomp AF008 ABS
LNP* Thermocomp* AF008 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
<br>@Thickness 3.20 mm
216 °F
<br>@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics LNP Thermocomp AF008 ABS (Asia Pacific)
LNP* Thermocomp* AF008 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
216 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP DF0081PI PC (Asia Pacific)
LNP* Thermocomp* DF0081PI is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High Modulus, good flatness, Non-Brominated & ..
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
<br>@Thickness 3.20 mm
216 °F
<br>@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP DX07350 PC (Asia Pacific)
Lexan *DX07350 resin is a glass filled, Non-brominated & Non-chlorinated flame retardant polycarbonate. High stiffness and good flow.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
<br>@Thickness 3.20 mm
216 °F
<br>@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP KB003RXZ Acetal Copolymer
LNP THERMOCOMP* KB003RXZ is a compound based on Acetal Copolymer resin containing 15% Glass Bead. Added features of this material include: Easy Release.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
<br>@Thickness 6.40 mm
216 °F
<br>@Thickness 0.252 in
ASTM D648
Samsung Cheil Industries Starex® GR-4015A ABS, Glass Filled
Information provided by Samsung Cheil Industries.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
216 °F
Annealed; ASTM D648
Techmer ES Plastiblend® ABS HH BK MB
Availability: North AmericaForms: PelletsFeatures: High Gloss and High Heat ResistanceAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
216 °F
ASTM D648
A. Schulman POLYFLAM™ FLP 3714 20% Glass Filled HDPE
DescriptionPolyfort® FLP 3714 is a 20% glass filled HDPE product. Information provided by A. Schulman.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
216 °F
Absolute Drying; ASTM-D648
Toyobo GLAMIDE® NB-5620S Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
216 °F
ASTM D648
Toyobo NB-5620S Nylon/Olefin Alloy, 15% Mineral Reinforced (DAM)
Features: 15% Mineral Reinforced, Light WeightInformation provided by Toyobo.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
216 °F
ASTM D648
A. Schulman POLYFLAM™ FLP 3714 20% Glass Filled HDPE
DescriptionPolyfort® FLP 3714 is a 20% glass filled HDPE product. Information provided by A. Schulman.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
216 °F
ISO 75-1,-2
Covestro Bayblend® T65 HG PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding, easy ..
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
216 °F
ASTM D648
Ensinger Tecaform™ HPV 13 Acetal Homopolymer - Extruded Products (POM)
Tecaform™ HPV 13 is a brown homopolymer acetal with an internal PTFE lubricant. Its low coefficient of friction, excellent PV values, toughness, wear resistance, and machinability make it an excep..
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
216 °F
ASTM D648
Beijing Chemical Industry KAIFA® M105N MPPO Resin
High flame retardant, Thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
216 °F
ASTM D648
Ashley Polymers Ashlene® R6041 Nylon 66, PTFE and Silicone Modified
Nylon 66 PTFE and Silicone modified for excellent wear characteristics and low friction.Data provided by the manufacturer
Copyright © lookpolymers.com All Rights Reserved