Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hybrid Plastics PK6U58.01 PEEK POSS® Flow Masterbatch

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Hybrid Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hybrid Plastics PK6U58.01 PEEK POSS® Flow Masterbatch.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
POSS® Flow masterbatches have shown success in reducing the melt viscosity of a variety of high temperature, difficult to process, thermoplastics. Hybrid Plastics offers such a solution for PEEK. PEEK POSS® Flow is a pellet masterbatch incorporating POSS® Flow in a PEEK carrier that can be used directly in the process or manufacturing stream. For injection molding applications, users will benefit from decreased molding pressures and increased flow for filling intricate and thin-walled parts. This leads to faster cycle times and less scrap. For extrusion applications, POSS® Flow will decrease screw torque, allowing for an increase in extrusion rate.Typical addition levels are 10 to 20%. Adding 20% to a high molecular weight PEEK nearly doubled the MFI and decreased extrusion torque by 28%. At loading levels of up to 50%, there is no appreciable decrease in mechanical properties, including modulus, HDT and elongation to break. PEEK POSS® Flow is especially effective in filled systems. POSS coats and interacts with most fillers (glass, mineral, clay, etc.), improving dispersion and significantly decreasing melt viscosity.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
Filler Content 10 - 50 %
10 - 50 %
Melt Flow 550 g/10 min

@Load 5.00 kg,
Temperature 380 °C
550 g/10 min

@Load 11.0 lb,
Temperature 716 °F
Descriptive Properties Value Comments
Color Opaque, light brown