Material Notes:
Mylar® RSX films are slightly hazy, tough, general-purpose films. They have a rough surface to provide ease of handling, good adhesion, and processability. They are used for a broad range of industrial applications.Mylar® RSX has balanced tensile properties and good dimensional stability.Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 140 %
140 %
ASTM D882A
Film Elongation at Break, TD 100 %
100 %
ASTM D882A
Film Tensile Strength at Break, MD 172 MPa
25000 psi
ASTM D882A
Film Tensile Strength at Break, TD 228 MPa
33000 psi
ASTM D882A
Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
Melting Point 254 °C
489 °F
Typical Mylar® via DSC
Shrinkage, MD 2.0 %

@Temperature 150 °C,
Time 1800 sec
2.0 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 0.70 %

@Temperature 150 °C,
Time 1800 sec
0.70 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Haze 14.4 %
14.4 %
ASTM D1003