Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Front Barrel Temperature = 200 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 200 °C
392 °F
Multibase TPSiV™ 3010-50A Thermoplastic Silicone Vulcanizate
These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced..
Front Barrel Temperature 200 - 210 °C
392 - 410 °F
Huntsman AVALON® 85 ABR Thermoplastic Polyurethane
Introduction: AVALON 85 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABR is part of the AVALON Performance Range and offers a premium soling ..
Front Barrel Temperature 200 - 220 °C
392 - 428 °F
Injection Molding
LG Chemical AF312A ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
Front Barrel Temperature 200 - 220 °C
392 - 428 °F
Injection Molding
LG Chemical HI100K ABS, High Impact
Feature: Injection Molding, High Impact, Good ProcessingApplication: Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical
Front Barrel Temperature 200 - 210 °C
392 - 410 °F
Injection Molding
LG Chemical HIPS 460AF PS, Flame Retardant
Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 25713-60-4, 84852-53-9 and 1309-64-4Information provided by LG Chemical
Front Barrel Temperature 200 - 220 °C
392 - 428 °F
LG Chemical LUCEL EC-605B Electrically Conductive POM, 5% Carbon Black Filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Front Barrel Temperature 200 - 220 °C
392 - 428 °F
LG Chemical LUCEL MR-320 Low Warpage POM, 20% Mineral Filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Front Barrel Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
LG Chemical LUPOL GP1000FC Flame Retardant PP
Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical
Front Barrel Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
LG Chemical LUPOL GP3200 PP+MF20%
Description: Injection Molding, PP+MF10%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
Front Barrel Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
LG Chemical LUPOL GP3202 PP+MF20%
Description: Injection Molding, PP+MF10%, General Purpose, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG..
Front Barrel Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
LG Chemical LUPOL HI5204S PP+MF20%, High Impact
Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical
Front Barrel Temperature 200 - 220 °C
392 - 428 °F
Injection Molding
LG Chemical SG175NS ABS, Super Surface Gloss, General Anti-Static
Feature: Injection Molding, Super Surface Gloss, General Anti-StaticApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical
Front Barrel Temperature 200 - 210 °C
392 - 410 °F
Lavergne VYSTYRENE PS 3901 High Impact Polystyrene
Vystyrene PS 3901 is a black impact modified polystyrene compound with balanced impact/stiffness properties designed for injection molding applicationsFeatures: -High resilience -Excellent process..
Front Barrel Temperature 200 - 220 °C
392 - 428 °F
Injection Molding
Stellarchem AB835EM-1 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed unconventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, completel..
Front Barrel Temperature 200 - 220 °C
392 - 428 °F
Injection Molding
Stellarchem AB860EM TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Front Barrel Temperature 200 - 220 °C
392 - 428 °F
Injection Molding
Stellarchem AB-860LG TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Front Barrel Temperature 200 - 220 °C
392 - 428 °F
Injection Molding
Stellarchem GP-9401 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Front Barrel Temperature 200 - 220 °C
392 - 428 °F
Injection Molding
Stellarchem GP-965B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Front Barrel Temperature 200 - 220 °C
392 - 428 °F
Injection Molding
Stellarchem LP-855 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Front Barrel Temperature 200 - 220 °C
392 - 428 °F
Injection Molding
Stellarchem MP-850 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Front Barrel Temperature 200 - 210 °C
392 - 410 °F
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS
VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 200 - 240 °C
392 - 464 °F
Injection Molding
Arkema Group KYNAR® 6000 HD Polyvinylidene Fluoride - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Front Barrel Temperature 200 - 240 °C
392 - 464 °F
Injection Molding
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Front Barrel Temperature 200 °C
392 °F
Injection
Alliance Polymers Zythane™ 7085AU Thermoplastic Polyurethane Elastomer
Zythane™ 7085UF is a UV stabilized polyether-based TPU specifically formulated for extrusion applications. It exhibits excellent abrasion resistance and toughness and has good hydrolytic stability,..
Front Barrel Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
LG Chemical LUPOL GP2300 PP+GF30%
Description: Injection Molding, PP+GF30%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical
Front Barrel Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
LG Chemical KEYFLEX TO1075AR Olefin Type TPE
Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7 and 14807-96-6Information provided by LG Chemical