Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Rear Barrel Temperature = 365 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Rear Barrel Temperature 185 - 207 °C
365 - 405 °F
Ineos Nova 50 High Performance Styrenic Enhanced Polystyrene  (discontinued **)
High strength crystal polystyrene, High heat crystal polystyrene, Custom colorsApplications: Injection molding or extrusion, Designed for applications requiring strength and high heat resistance whe..
Rear Barrel Temperature 185 - 207 °C
365 - 405 °F
Ineos Nova 879 High Performance Styrenic Enhanced Polystyrene  (discontinued **)
High heat crystal polystyrene, Color stable, Custom colorsApplications: Injection molding, Designed for applications requiring high strength, high heat resistance, and color stabilityPerformance gra..
Rear Barrel Temperature 185 - 195 °C
365 - 383 °F
Huntsman AVALON® 98 AE Thermoplastic Polyurethane
Introduction: AVALON 98 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 98 AE is part of the AVALON Perform Range and offers a premium soiling materi..
Rear Barrel Temperature 185 - 205 °C
365 - 401 °F
Injection Molding
LG Chemical KEYFLEX BT 1033D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
Rear Barrel Temperature 185 - 195 °C
365 - 383 °F
Huntsman AVALON® 85 AE Thermoplastic Polyurethane
Introduction: AVALON 85 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 85 AE is part of the AVALON Perform Range and offers a premium soiling materi..
Rear Barrel Temperature 185 - 195 °C
365 - 383 °F
Huntsman AVALON® 92 AE Thermoplastic Polyurethane
Introduction: AVALON 92 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 92 AE is part of the AVALON Perform Range and offers a premium soiling materi..
Rear Barrel Temperature 185 - 195 °C
365 - 383 °F
Huntsman AVALON® 95 AE Thermoplastic Polyurethane
Introduction: AVALON 95 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AE is part of the AVALON Perform Range and offers a premium soiling materi..
Rear Barrel Temperature 185 - 195 °C
365 - 383 °F
Huntsman AVALON® 95 AEU Thermoplastic Polyurethane
Introduction: AVALON 95 AEU is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AEU is part of the AVALON Perform Range and offers a premium soiling mate..
Rear Barrel Temperature 185 - 205 °C
365 - 401 °F
Chi Mei Acryrex® CM-205 PMMA
High heat injection grade. It can resist high temperature. High mechanical strength.Applications: The indicator cover of scooter and automobile/sun glasses/digital watch cover.Features:Good Weather ..
Rear Barrel Temperature 185 - 200 °C
365 - 392 °F
Chi Mei Acryrex® CM-207 PMMA
Features:General PurposeGood Weather ResistanceHigh GlossHigh Heat ResistanceHigh StrengthMedium ViscosityUses: Automotive Interior PartsBathroom AccessoriesContainersCosmeticsHousehold GoodsKnobsRo..
Rear Barrel Temperature 185 - 199 °C
365 - 390 °F
ExxonMobil Santoprene® 8201-80 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..
Rear Barrel Temperature 185 °C
365 °F
Injection
Alliance Polymers Viprene™ G90A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G90A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Rear Barrel Temperature 185 °C
365 °F
Injection
Alliance Polymers Viprene™ G90A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G90A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Rear Barrel Temperature 185 °C
365 °F
Injection
Alliance Polymers Zythane™ 4090A Thermoplastic Polyurethane Elastomer
Zythane™ 4090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Rear Barrel Temperature 185 °C
365 °F
Injection
Alliance Polymers Zythane™ 5090A Thermoplastic Polyurethane Elastomer
Zythane™ 5090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Rear Barrel Temperature 185 °C
365 °F
Injection
Alliance Polymers Zythane™ 6090A Thermoplastic Polyurethane Elastomer
Zythane™ 6090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Rear Barrel Temperature 185 °C
365 °F
Injection
Alliance Polymers Zythane™ 7085AF Thermoplastic Polyurethane Elastomer
Zythane™ 7085AF is a FR polyether-based TPU specifically formulated with non-halogenated flame retardants for extrusion applications with ease of processing. It exhibits excellent abrasion resistan..
Rear Barrel Temperature 185 °C
365 °F
Injection
Alliance Polymers Zythane™ 7090A Thermoplastic Polyurethane Elastomer
Zythane™ 7090A is a polyether-based TPU specifically formulated for extrusion molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good hydroly..
Rear Barrel Temperature 185 °C
365 °F
ExxonMobil Santoprene® 223-50 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
Copyright © lookpolymers.com All Rights Reserved