LATI Latishield 36/SP-05A ABS, Steel Fiber Reinforced

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled
Manufacturer LATI
Trade Name Latishield
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Latishield 36/SP-05A ABS, Steel Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
EMI shielding product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
Linear Mold Shrinkage, Flow 0.0065 - 0.0085 cm/cm
0.0065 - 0.0085 in/in
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm
0.0070 - 0.0090 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.0 MPa
5080 psi
Elongation at Break 3.5 %
3.5 %
Elongation at Yield 2.0 %
2.0 %
Tensile Modulus 2.40 GPa
348 ksi
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
Vicat Softening Point 85.0 °C

@Load 5.00 kg
185 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Surface Resistance 50 ohm
50 ohm
Processing Properties Metric English Comments
Melt Temperature 210 - 250 °C
410 - 482 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Descriptive Properties Value Comments
Electromagnetic reflection 92 dB
ISO Shrinkage - Pressure 60 MPa