Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kolon KOPA® KN333HI4 High Impact Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer Kolon
Trade Name Kopa®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Kolon KOPA® KN333HI4 High Impact Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstanding self lubrication and abrasion resistance, excellent chemical & weather resistance, high usage temperatureInformation provided by US distributor, API-Kolon.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
DIN 53479; ASTM D792
Water Absorption 0.90 %
0.90 %
DIN 53475; ASTM D570
Linear Mold Shrinkage 0.017 - 0.020 cm/cm
0.017 - 0.020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
DIN 53505; ASTM D785
Tensile Strength, Ultimate 53.9 MPa
7820 psi
DIN 53455; ASTM D638
Elongation at Break 85 %
85 %
DIN 53455; ASTM D638
Flexural Yield Strength 68.6 MPa
9960 psi
DIN 53455; ASTM D790
Flexural Modulus 1.57 GPa
228 ksi
DIN 53452; ASTM D790
Izod Impact, Notched NB
NB
DIN 53453; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 60.0 µm/m-°C

@Temperature 20.0 °C
33.3 µin/in-°F

@Temperature 68.0 °F
DIN 53752; ASTM D696
Melting Point 255 °C
491 °F
DIN 53736; ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
392 °F
DIN 53461; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
DIN 53461; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 3.1

@Frequency 1e+6 Hz
3.1

@Frequency 1e+6 Hz
ASTM D150/DIN 53483
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149/DIN 53481
Arc Resistance 125 sec
125 sec
ASTM D495