Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. 80 Battery Flux

Category Fluid
Manufacturer Indium Corporation of America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. 80 Battery Flux.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FeaturesLow fumingMinimal residueLow smokeLow evaporation80 Battery Flux is specially formulated for cast-on-strap manufacturing of batteries. This flux offers a wide process window at various temperatures and an extended life80 Battery Flux does not contain any chlorides, heavy metals or organic acids that could affect the long-term life of the battery.Characteristics:Color - light amberInformation provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc

@Temperature 25.0 °C
1.10 g/cc

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Flash Point >= 93.3 °C
>= 200 °F
TCC
Descriptive Properties Value Comments
Pounds per Gallon 9.17
Users viewing this material also viewed the following: