Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® 980LS Nylon 612

Category Polymer , Thermoplastic , Nylon , Nylon 612 , Nylon 612, Unreinforced
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 980LS Nylon 612.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A general purpose 612 nylon for injection molding, lubricated and heat stabilized. These resins are noted for their low moisture absorption and excellent dimensional stability.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Water Absorption 0.37 %
0.37 %
24 hrs; ASTM D570
Water Absorption at Saturation 3.0 %
3.0 %
ASTM D570
Linear Mold Shrinkage 0.011 cm/cm
0.011 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Ultimate 61.0 MPa
8850 psi
ATSM D638
Elongation at Break 90 %
90 %
ASTM D638
Flexural Modulus 1.90 GPa
276 ksi
ASTM D790
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 213 °C
415 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 164 °C
327 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
ASTM D648
Brittleness Temperature -126 °C
-195 °F
ASTM D746
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Dielectric Constant 3.5

@Frequency 1e+6 Hz
3.5

@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
ASTM D150
Users viewing this material also viewed the following: