UL 360 jacket compound. 105°C air; 60°C oil.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.26 - 1.30 g/cc
1.26 - 1.30 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 77 - 83
77 - 83
delayed; ASTM D-2240
Tensile Strength, Yield 17.9 MPa
2600 psi
ASTM D-638
Elongation at Yield 350 %
350 %
ASTM D-638
100% Modulus 0.00931 GPa
1.35 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -32.0 °C
-25.6 °F
ASTM D-746
Oxygen Index 23 %
23 %
ASTM D-638