Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Materion Beryllium Copper Alloy 165 Rod and Bar; AT (TF00) Temper; over 76 mm (UNS C17000)

Category Metal , Nonferrous Metal , Beryllium Alloy , Copper Alloy
Manufacturer Materion Corporation (former Brush Wellman)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Materion Beryllium Copper Alloy 165 Rod and Bar; AT (TF00) Temper; over 76 mm (UNS C17000).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Physical Properties Metric English Comments
Density 8.41 g/cc
0.304 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 32 - 39
32 - 39
Tensile Strength, Ultimate 1030 - 1320 MPa
149000 - 191000 psi
Tensile Strength, Yield 860 - 1070 MPa
125000 - 155000 psi
Elongation at Break 3.0 - 10 %
3.0 - 10 %
Modulus of Elasticity 131 GPa
19000 ksi
Thermal Properties Metric English Comments
CTE, linear 17.0 µm/m-°C

@Temperature 20.0 - 200 °C
9.44 µin/in-°F

@Temperature 68.0 - 392 °F
Thermal Conductivity 105 W/m-K
729 BTU-in/hr-ft²-°F
Melting Point 870 - 980 °C
1600 - 1800 °F
Solidus 870 °C
1600 °F
Liquidus 980 °C
1800 °F
Component Elements Properties Metric English Comments
Beryllium, Be 1.6 - 1.79 %
1.6 - 1.79 %
Co + Ni >= 0.20 %
>= 0.20 %
Co + Ni + Fe <= 0.60 %
<= 0.60 %
Copper, Cu 98 %
98 %
as balance
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000610 - 0.00000780 ohm-cm
0.00000610 - 0.00000780 ohm-cm
22-28% IACS Conductivity