Overview of materials for Nylon 6, Stainless Steel Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Stainless Steel Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Nylon 6, Stainless Steel Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.20 - 4.00 g/cc
0.0434 - 0.145 lb/in³
Average value: 1.75 g/cc Grade Count:7
Filler Content 7.00 - 15.0 %
7.00 - 15.0 %
Average value: 10.7 % Grade Count:3
Water Absorption 1.00 - 1.40 %
1.00 - 1.40 %
Average value: 1.16 % Grade Count:5
Linear Mold Shrinkage 0.00200 - 0.0150 cm/cm
0.00200 - 0.0150 in/in
Average value: 0.00693 cm/cm Grade Count:7
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
Average value: 117 Grade Count:3
Tensile Strength, Ultimate 25.0 - 82.7 MPa
3630 - 12000 psi
Average value: 60.5 MPa Grade Count:4
Tensile Strength, Yield 131 - 138 MPa
19000 - 20000 psi
Average value: 136 MPa Grade Count:3
Elongation at Break 0.500 - 10.0 %
0.500 - 10.0 %
Average value: 5.86 % Grade Count:7
Modulus of Elasticity 2.76 - 7.50 GPa
400 - 1090 ksi
Average value: 4.12 GPa Grade Count:4
Flexural Yield Strength 82.7 - 193 MPa
12000 - 28000 psi
Average value: 151 MPa Grade Count:6
Flexural Modulus 2.41 - 7.58 GPa
350 - 1100 ksi
Average value: 5.37 GPa Grade Count:7
Izod Impact, Notched 0.534 - 0.854 J/cm
1.00 - 1.60 ft-lb/in
Average value: 0.667 J/cm Grade Count:6
Izod Impact, Unnotched 8.01 - 9.61 J/cm
15.0 - 18.0 ft-lb/in
Average value: 8.54 J/cm Grade Count:3
Thermal Properties Metric English Comments
CTE, linear 54.0 µm/m-°C
30.0 µin/in-°F
Average value: 54.0 µm/m-°C Grade Count:3
Deflection Temperature at 1.8 MPa (264 psi) 82.2 - 210 °C
180 - 410 °F
Average value: 159 °C Grade Count:5
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:3
Electrical Properties Metric English Comments
Electrical Resistivity 1.00 - 100 ohm-cm
1.00 - 100 ohm-cm
Average value: 21.3 ohm-cm Grade Count:6
Surface Resistance 10.0 - 1.00e+6 ohm
10.0 - 1.00e+6 ohm
Average value: 335000 ohm Grade Count:6
Static Decay 2.00 sec
2.00 sec
Average value: 2.00 sec Grade Count:6
Shielding Effectiveness 50.0 dB
50.0 dB
Average value: 50.0 dB Grade Count:3
Processing Properties Metric English Comments
Processing Temperature 221 - 271 °C
430 - 520 °F
Average value: 246 °C Grade Count:3
Mold Temperature 54.4 - 93.3 °C
130 - 200 °F
Average value: 73.5 °C Grade Count:4
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:3