Eurotec
Trade Name Tecotek®
Trade Name :
Tecotek®
Product List
Category
Polycarbonate/ABS Alloy, Unreinforced
,
Polycarbonate, 20% Glass Filled
,
Polycarbonate, Impact Modified
,
Polycarbonate, Unreinforced, Flame Retardant
,
Polycarbonate, UV Stabilized
,
Polycarbonate, 10% Glass Filled
,
Polycarbonate, 30% Glass Filled
Manufacturer
Eurotec
Tips:
Up to 50 items displayed.
PRODUCT NO.
Category
Eurotec® Tecotek® BC40 UF45 NL CE PC/ABS, unfilled, heat & UV stabilized, natural, easy flow grade
Polycarbonate/ABS Alloy, Unreinforced
Eurotec® Tecotek® BC40 UF65 NL CE PC/ABS, unfilled, heat & UV stabilized, natural, standard grade
Polycarbonate/ABS Alloy, Unreinforced
Eurotec® Tecotek® BC40 UF85 NL CE PC/ABS, unfilled, heat & UV stabilized, natural, high heat grade
Polycarbonate/ABS Alloy, Unreinforced
Eurotec® Tecotek® BC43 UF65 NL CE PC/ABS, unfilled, heat & UV stabilized, natural, standard grade
Polycarbonate/ABS Alloy, Unreinforced
Eurotec® Tecotek® PC30 GR20 GR003 ZG20 PC, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), grey RAL 7035
Polycarbonate, 20% Glass Filled
Eurotec® Tecotek® PC30 NL RX PC, unfilled, improved flow & low temperature impact, natural
Polycarbonate, Impact Modified
Eurotec® Tecotek® PC30 NL TD 700 PC, unfilled, flame retardant - halogen (RoHS compliant), impact modified, natural
Polycarbonate, Impact Modified
Eurotec® Tecotek® PC30 NL VB03 PC, unfilled, UV stabilized, high impact, natural
Polycarbonate, Impact Modified
Eurotec® Tecotek® PC40 GR10 NL PC, 10% glass fiber reinforced, natural
Polycarbonate, 10% Glass Filled
Eurotec® Tecotek® PC40 GR20 NL PC, 20% glass fiber reinforced, natural
Polycarbonate, 20% Glass Filled
Eurotec® Tecotek® PC40 GR30 NL PC, 30% glass fiber reinforced, natural
Polycarbonate, 30% Glass Filled
Eurotec® Tecotek® PC40 NL FA70 PC, unfilled, flame retardant - (RoHS compliant), natural
Polycarbonate, Unreinforced, Flame Retardant
Eurotec® Tecotek® PC40 NL VB02 PC, unfilled, UV stabilized, high impact, natural
Polycarbonate, Impact Modified
Eurotec® Tecotek® PC43 GR003 TD70 PC, unfilled, flame retardant - halogen (RoHS compliant), impact modified, light grey
Polycarbonate, Impact Modified
Eurotec® Tecotek® PC43 GR10 BK002 PC, 10% glass fiber reinforced, black
Polycarbonate, 10% Glass Filled
Eurotec® Tecotek® PC43 GR20 BK002 PC, 20% glass fiber reinforced, black
Polycarbonate, 20% Glass Filled
Eurotec® Tecotek® PC43 GR30 BK002 PC, 30% glass fiber reinforced, black
Polycarbonate, 30% Glass Filled
Eurotec® Tecotek® PC44 GR003 ZG70 PC, unfilled, flame retardant - halogen (RoHS compliant), light grey
Polycarbonate, Unreinforced, Flame Retardant
Eurotec® Tecotek® PC44 GR10 GR003 ZG70 PC, 10% glass fiber reinforced, flame retardant - halogen (RoHS compliant), light grey
Polycarbonate, 10% Glass Filled
Eurotec® Tecotek® PC50 GR10 GR053 FA20 PC, 10% glass fiber reinforced, flame retardant - halogen (RoHS compliant), grey RAL 9002
Polycarbonate, 10% Glass Filled