Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 68.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 68.0 µm/m-°C

@Thickness 1.00 mm,
Temperature 125 - 175 °C
37.8 µin/in-°F

@Thickness 0.0394 in,
Temperature 257 - 347 °F
ASTM E831-06
NeXolve CORIN XLS Polyimide
Resistant to radiation and atomic oxygen erosion. NeXolve’s CORIN XLSPolyimide is a colorless, clear, organic/inorganic sprayable nanocomposite that is resistant to radiation and atomic oxygen eros..
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy 1080-70 Polycarbonate Resin
Description: LUPOY PC 1080-70 resin is designed for optical media discs applications. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Ch..
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy 1200-03 Polycarbonate Resin
Description: LUPOY PC 1200-03 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy 1201-10 Polycarbonate Resin
Description: LUPOY PC 1201-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy 1201-15 Polycarbonate Resin
Description: LUPOY PC 1201-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy 1300-15 Polycarbonate Resin
Description: LUPOY PC 1300-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy 1300-22 Polycarbonate Resin
Description: LUPOY PC 1300-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy 1301-12 Polycarbonate Resin
Description: LUPOY PC 1301-12 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy 1261-03 Polycarbonate Resin
Description: LUPOY PC 1261-03 resin is designed for extrusion blow molding(EBM) and injection stretch blow molding (ISBM) products. It exhibits an excellent physical property balance of heat resista..
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy 1301V-10 Polycarbonate Resin
Description: LUPOY PC 1301V-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength..
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy 1303EP-22 Polycarbonate Resin
Description: LUPOY PC 1303EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy 1603-03 Polycarbonate Resin
Description: LUPOY PC 1603-03 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics: ..
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy 1621-02 Polycarbonate Resin
Description: LUPOY PC 1621-02 resin is designed for large injection stretch blow molding and extrusion blow molding parts. It exhibits an excellent physical property balance of heat resistance, tran..
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy NF1005F 03R Polycarbonate Resin
Description: LUPOY NF 1005F03R, eco-friendly UL94 V0/1.5 mm, is designed for extrusion products. It combines an excellent physical property balance of heat resistance, transparency and impact streng..
CTE, linear 68.0 µm/m-°C
37.8 µin/in-°F
DIN 52328
Isoflon PMMA Polymethyl-methacrylate
Products with good mechanical performances under friction and good dimensional stability, notably in moist environmentsVery rigid, hardHigh machining precisionInformation provided by Isoflon.
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy 1201-22 Polycarbonate Resin
Description: LUPOY PC 1201-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy 1300-10 Polycarbonate Resin
Description: LUPOY PC 1300-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy 1300-12 Polycarbonate Resin
Description: LUPOY PC 1300-12 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy 1302-10 Polycarbonate Resin
Description: LUPOY PC 1302-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy 1302EP-30 Polycarbonate Resin
Description: LUPOY PC 1302EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy 1302HP-09 Polycarbonate Resin
Description: LUPOY PC 1302HP-09 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics..
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy 1302HP-21 Polycarbonate Resin
Description: LUPOY PC 1302HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
CTE, linear 68.0 µm/m-°C

@Temperature 20.0 °C
37.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Ineos ABS Lustran® SAN Sparkle Highest-Clarity
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy 1303-07 Polycarbonate Resin
Description: LUPOY PC 1303-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy 1303-10 Polycarbonate Resin
Description: LUPOY PC 1303-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
LG Chemical Lupoy 1303EP-30 Polycarbonate Resin
Description: LUPOY PC 1303EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
CTE, linear 68.0 µm/m-°C

@Temperature -40.0 - 35.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 95.0 °F
ASTM D696
MRC Polymers NAXELLâ„¢ PC110-919 General Purpose Polycarbonate, Medium High MFR
Polycarbonate for colorable productsMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedCan be clear to color matchedNot for products that req..
CTE, linear 68.0 µm/m-°C

@Temperature 20.0 °C
37.8 µin/in-°F

@Temperature 68.0 °F
Cotronics Duralco™ 4703 Adhesive and Tooling Compound
High temperature resin reinforced with ceramic and metallic fibers and particles, resulting in high thermal stability. Easily machined to close tolerances and will repair and rebuild worn or cracke..
CTE, linear 68.0 µm/m-°C

@Temperature 20.0 °C
37.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Covestro Bayflex® 190 Polyurethane Elastomeric RIM, 20% Mineral Filled, MDI-based 2-Component Liquid System
0.150 in. thickness. Calcium Silicate filled. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was se..
CTE, linear 68.0 µm/m-°C

@Temperature 20.0 °C
37.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Devcon Plastic Steel® Liquid (B) Epoxy
General Repair EpoxyComments: Steel-filled liquid epoxy can be cast over models for accurate detail reproduction when making holding fixtures, light-gauge forming dies and molds. Hardens in about a..
Copyright © lookpolymers.com All Rights Reserved