Material Notes:
Material Description: A two component, room temperature curing, general and structural grade epoxy. It can be used for adhesive, sealing, and encapsulating applications in medical, xray device, filtration, opto-electronics, and PCB industries. It is a black version of EPO-TEK® 730 Unfilled.Information Provided by Epoxy Technology
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
Part B
1.17 g/cc
1.17 g/cc
Part A
Viscosity 10000 - 14000 cP

@Temperature 23.0 °C
10000 - 14000 cP

@Temperature 73.4 °F
20 rpm
Mechanical Properties Metric English Comments
Hardness, Shore D 76
76
Tensile Modulus 0.896 GPa
130 ksi
Storage
Shear Strength >= 13.8 MPa
>= 2000 psi
Lap
>= 23.4 MPa
>= 3400 psi
Die
Thermal Properties Metric English Comments
CTE, linear 61.0 µm/m-°C
33.9 µin/in-°F
Below Tg
192 µm/m-°C
107 µin/in-°F
Above Tg
Maximum Service Temperature, Air 150 °C
302 °F
Continuous
250 °C
482 °F
Intermittent
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Continuous
-55.0 °C
-67.0 °F
Intermittent
Glass Transition Temp, Tg >= 50.0 °C
>= 122 °F
Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Decomposition Temperature 343 °C
649 °F
Degradation Temperature
Optical Properties Metric English Comments
Transmission, Visible <= 2.0 %

@Wavelength 300 - 960 nm
<= 2.0 %

@Wavelength 300 - 960 nm
Spectral
<= 5.0 %

@Wavelength 980 - 1260 nm
<= 5.0 %

@Wavelength 980 - 1260 nm
Spectral
Electrical Properties Metric English Comments
Volume Resistivity <= 4.00e+13 ohm-cm
<= 4.00e+13 ohm-cm
Dielectric Constant 3.24

@Frequency 1000 Hz
3.24

@Frequency 1000 Hz
Dissipation Factor 0.0090

@Frequency 1000 Hz
0.0090

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 100 °C
0.500 hour

@Temperature 212 °F
minimum
1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
minimum
Pot Life 60 min
60 min
Shelf Life 12.0 Month

@Temperature 25.0 °C
12.0 Month

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Black
Part A
Clear Yellow
Part B
Consistency Pourable liquid
Mix Ratio By Weight 1:1
Number of Components Two
Weight Loss 1.01%
200°C