Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792, ISO 1183
Water Absorption 0.15 %
<br>@Temperature 23.0 °C
0.15 %
<br>@Temperature 73.4 °F
24h; ASTM D570, ISO 62
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Melt Index of Compound 15 - 20 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
15 - 20 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
ASTM D1238, ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell L 70
70
ASTM D785, ISO 2039/2
Tensile Strength, Yield 50.0 MPa
7250 psi
ASTM D638, ISO R527
Elongation at Break >= 50 %
>= 50 %
ASTM D638, ISO R527
Flexural Strength 80.0 MPa
11600 psi
ASTM D790, ISO 178
Flexural Modulus 2.20 GPa
319 ksi
ASTM D790, ISO 178
Izod Impact, Notched >= 0.800 J/cm
<br>@Thickness 3.20 mm,<br> Temperature -40.0 °C
>= 1.50 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature -40.0 °F
ASTM D256, ISO 180/4a
>= 2.50 J/cm
<br>@Thickness 3.20 mm,<br> Temperature 0.000 °C
>= 4.68 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature 32.0 °F
ASTM D256, ISO 180/4a
>= 4.00 J/cm
<br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
>= 7.49 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature 73.4 °F
ASTM D256, ISO 180/4a
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 110 °C
230 °F
20000 h; VDE 0304/P2-1, IEC 216
115 °C
239 °F
5000 h; VDE 0304/P2-1, IEC 216
135 °C
275 °F
few hours; VDE 0304/P2-1, IEC 216
Hot Ball Pressure Test >= 128 °C
>= 262 °F
BS 3456, IEC 335
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
ASTM D648, ISO 75
Vicat Softening Point 138 - 145 °C
<br>@Load 5.00 kg
280 - 293 °F
<br>@Load 11.0 lb
120°C/min; ASTM D1525/B, ISO 306/B
150 - 155 °C
<br>@Load 0.999 kg
302 - 311 °F
<br>@Load 2.20 lb
120°C/min; ASTM D1525/A, ISO 306/A
Flammability, UL94 V-2
<br>@Thickness 1.60 mm
V-2
<br>@Thickness 0.0630 in
V-2
<br>@Thickness 3.20 mm
V-2
<br>@Thickness 0.126 in
Glow Wire Test 750 °C
<br>@Thickness 3.20 mm
1380 °F
<br>@Thickness 0.126 in
VDE 0471/P2-4, IEC 695
750 °C
<br>@Thickness 2.00 mm
1380 °F
<br>@Thickness 0.0787 in
VDE 0471/P2-4, IEC 695
Electrical Properties Metric English Comments
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
ASTM D257, IEC 93
Dielectric Constant 3.0
<br>@Frequency 1000 Hz
3.0
<br>@Frequency 1000 Hz
ASTM D150, IEC 250
Dielectric Strength 35.0 kV/mm
889 kV/in
ASTM D149, IEC 243
Dissipation Factor 0.0010
<br>@Frequency 1000 Hz
0.0010
<br>@Frequency 1000 Hz
ASTM D150, IEC 250
Comparative Tracking Index 180 V
180 V
VDE 0303-P1, IEC 112