| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Zytel® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | DuPont Performance Polymers Zytel® ST801AHS BK010 Nylon 66
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.09 g/cc | 0.0394 lb/in³ | DAM; ISO 1183 |
| Moisture Absorption | 2.00 % @Thickness 2.00 mm |
2.00 % @Thickness 0.0787 in |
DAM; Sim. to ISO 62 |
| Water Absorption at Saturation | 1.1 % | 1.1 % | DAM; Immersion 24h; ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.023 cm/cm | 0.023 in/in | DAM; ISO 294-4 2577 |
| Linear Mold Shrinkage, Transverse | 0.015 cm/cm | 0.015 in/in | DAM; ISO 294-4 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 69 | 69 | 50%RH; ISO 2039-2 |
| 107 | 107 | DAM; ISO 2039-2 | |
| Tensile Strength, Yield | 39.0 MPa | 5660 psi | 50%RH; ISO 527-1/-2 |
| 47.0 MPa | 6820 psi | DAM; ISO 527-1/-2 | |
| Elongation at Break | 50 % | 50 % | DAM; Nominal; ISO 527-1/-2 |
| >= 50 % | >= 50 % | 50%RH; Nominal; ISO 527-1/-2 | |
| Elongation at Yield | 4.0 % | 4.0 % | DAM; ISO 527-1/-2 |
| 39 % | 39 % | 50%RH; ISO 527-1/-2 | |
| Tensile Modulus | 1.096 GPa | 159.0 ksi | 50%RH; ISO 527-1/-2 |
| 1.80 GPa | 261 ksi | DAM; ISO 527-1/-2 | |
| Flexural Modulus | 0.832 GPa | 121 ksi | 50%RH; ISO 178 |
| 1.90 GPa | 276 ksi | DAM; ISO 178 | |
| Izod Impact, Notched (ISO) | 71.0 kJ/m² | 33.8 ft-lb/in² | DAM; ISO 180/1A |
| 17.0 kJ/m² @Temperature -40.0 °C |
8.09 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A | |
| 19.0 kJ/m² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | NB | NB | DAM; ISO 180/1U |
| Charpy Impact Unnotched | NB | NB | DAM; ISO 179/1eU |
| Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | DAM; ISO 179/1eA |
| 10.5 J/cm² | 50.0 ft-lb/in² | 50%RH; ISO 179/1eA | |
| 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA | |
| 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 140 µm/m-°C | 77.8 µin/in-°F | DAM; ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 120 µm/m-°C | 66.7 µin/in-°F | DAM; ISO 11359-1/-2 |
| Melting Point | 262 °C | 504 °F | DAM; 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 147 °C | 297 °F | DAM; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 61.0 °C | 142 °F | DAM; ISO 75-1/-2 |
| Flammability, UL94 | HB @Thickness 0.800 mm |
HB @Thickness 0.0315 in |
DAM; IEC 60695-11-10 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Part Marking Code | >PA66-HI< | ISO 11469 |
| Processing | Injection Moulding | |
| Regional Availability | Asia Pacific | |
| Europe | ||
| Global | ||
| Near East/Africa | ||
| North America | ||
| South and Central America | ||
| Resin Identification | PA66-HI |