| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
| SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
| SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer (Asia Pacific) Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
| SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
| SABIC Innovative Plastics LNP Faradex MS003XXC PP (Europe-Africa-Middle East) LNP* Faradex* MS003XXC is a compound based on Polypropylene resin containing Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding.This data was supplied by SABIC-IP for.. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
| SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | ISO 180/1A |
| Lucite International Diakon® Rapide CLG 910B Enhanced Molding Acrylic Polymer Specially designed to reduce injection molding cycle times and therefore provide production cost benefits.Information provided by Lucite International |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | 80*10*4; ISO 180/1A |
| SABIC Innovative Plastics LNP LUBRICOMP DP0039EF PC (Asia Pacific) LNP* Lubricomp* DP0039EF is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | 80*10*4; ISO 180/1A |
| SABIC Innovative Plastics LNP LUBRICOMP DX94375H PC LNP* LUBRICOMP* DX94375H is a compound based on Polycarbonate resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm, r=0.25; V-notch; ISO 180/1A |
| SYNTHOS Forsan® 449 Acrylonitrile Butadiene Styrene (ABS) High flow, high gloss, suitable for electroplating.Applications: General purpose, intricate and thin-walled productsHousehold appliances, vacuum cleaners, heels, toys, fan grilles, etc.Synthos was f.. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | ISO 180/1eA |
| Solvay TECHNYL® B 216 V30 Black 3 N PA66, 30% glass fiber, Conditioned Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 216 V30 is used in all sectors of in.. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | ISO 180/1eA |
| Solvay TECHNYL® B 218L V30 Black 44 N PA66, 30% glass fiber, Conditioned Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistance.Available in: Asia Pacific, Europe and Latin AmericaProdu.. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | ISO 180/1eA |
| Solvay TECHNYLSTARâ„¢ S 216 V30 PA6, 30% glass filled, Conditioned Description: TECHNYL STAR TM Polyamide, reinforced with 30% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific, Europe and North AmericaPr.. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | 80*10*4; ISO 180/1A |
| SABIC Innovative Plastics LNP LUBRILOY RX05498 PA 66 LNP LUBRILOY* RX05498 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: High Impact, Wear Resistant. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | 80*10*4; ISO 180/1A |
| SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | 80*10*4; ISO 180/1A |
| SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Europe-Africa-Middle East) LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | 80*10*4; ISO 180/1A |
| SABIC Innovative Plastics LNP THERMOCOMP QF00A PA 6/10 (Europe-Africa-Middle East) LNP* Thermocomp* QF00A is a compound based on Nylon 6/10 resin containing Glass Fiber. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
| SABIC Innovative Plastics LNP Thermocomp RF00CS PA 66 LNP* Thermocomp* RF00CS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re.. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | 80*10*4; ISO 180/1A |
| SABIC Innovative Plastics LNP THERMOCOMP RF00CSXS PA 66 (Asia Pacific) LNP* Thermocomp* RF00CSXS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | 80*10*4; ISO 180/1A |
| SABIC Innovative Plastics LNP THERMOCOMP RF00CSXZ PA 66 LNP* THERMOCOMP* RF00CSXZ is a compound based on Recycled Nylon 66 resin containing 60% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | ISO 180 |
| Tisan TISLAMID® 66 30% Glass Filled Impact Modified, Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | ASTM D256 |
| Tipco Tipcolene® SEB 400 - 40% Chemically Coupled Glass Fibers Polypropylene Homopolymer with High Heat Stability 40% Chemically Coupled Glass Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | ISO 180 |
| Polyram PlusTek PB202G50BK39 Nylon 6, 50% Glass Fiber Reinforced, UV and Heat Stabilized 50% Glass fiber reinforced, UV and heat stabilized Nylon 6. Approved and listed by NSF/ANSI 61 International.Information provided by Polyram. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | Low Temp; ISO 180/1eA |
| Lubrizol ESTALOC® T5160 Ether-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | ISO 180/1A |
| Chi Mei Polylac® PA-737 ABS - High Flow High flow, medium impact |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² | 9.04 ft-lb/in² | ISO 180/1A |
| Chi Mei Polylac® PA-777B ABS - High Heat High Heat Impact |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
| BASF Ultramid® B3EG7 35% Glass Filled PA6 (Dry) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
| BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Dry) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
| SABIC Innovative Plastics Cycolac® DL100LG ABS (Europe-Africa-Middle East) Cycolac DL100LG is a low gloss, high heat, high impact ABS/PC blend with low emission |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 0.000 °C |
9.04 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
| SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only. |
|||
| Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
| SABIC Innovative Plastics LNP Stat-kon MDM40 PP LNP* Stat-Kon* MDM40 is a compound based on Polypropylene resin containing Mica and Carbon. Characteristics are Statically Conductive.This data was supplied by SABIC-IP for the Americas region. |
|||