3A Composites Core Materials AIREX® T90.60 Easy Processing Structural FST Foam

Category Other Engineering Material , Composite Core Material , Polymer , Thermoplastic
Manufacturer 3A Composites Core Materials
Trade Name AIREX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3A Composites Core Materials AIREX® T90.60 Easy Processing Structural FST Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigue, is chemically stable, UV-resistant and has negligible water absorption. It is thermally stable during high temperature processing and post curing without after expansion or outgassing. T90 is designed for easy use with all resin systems and processing technologies. AIREX® T90 is the ideal core material for structural sandwich applications requiring high fire resistance.CharacteristicGood FST Properties (FAR 25.853; NF 16.101; DIN 5510)Excellent fatigue strengthEasy to process with all types of resin and lamination processesExcellent long term thermal stability up to 100°C (212°F)Best thermal stability in process up to 150°C (302 °F)High compression strength and modulusVery low variance of the mechanical valuesGood adhesion (skin-to-core bond)Excellent chemical stabilityNo water absorptionNo after-expansion, no outgassingApplicationsRoad and Rail: Floors, sidewalls, font ends, interiors, roofs, engine coversMarine: Decks, interiors, superstructure Industrial: Cover, containers, x-ray tables, sporting goodArchitecture and Construction: Roofs, claddings, domes, portable building
Physical Properties Metric English Comments
Density 0.0650 g/cc
0.00235 lb/in³
average; ISO 845
0.0600 - 0.0700 g/cc
0.00217 - 0.00253 lb/in³
typical range; ISO 845
Mechanical Properties Metric English Comments
Tensile Strength >= 1.20 MPa
>= 174 psi
perpendicular to plane; ASTM C297
1.50 MPa
218 psi
average; perpendicular to plane; ASTM C297
Elongation at Break >= 8.0 %
>= 8.0 %
shear; ISO 1922
12 %
12 %
average; shear; ISO 1922
Tensile Modulus >= 0.0700 GPa
>= 10.2 ksi
perpendicular to plane; ASTM C297
0.0850 GPa
12.3 ksi
average; perpendicular to plane; ASTM C297
Compressive Strength >= 0.700 MPa
>= 102 psi
perpendicular to plane; ISO 844
0.800 MPa
116 psi
average; perpendicular to plane; ISO 844
Compressive Modulus >= 0.0350 GPa
>= 5.08 ksi
perpendicular to plane; DIN 53421
0.0500 GPa
7.25 ksi
average; perpendicular to plane; DIN 53421
Shear Modulus >= 10.5 GPa
>= 1520 ksi
ASTM C393
12.0 GPa
1740 ksi
average; ASTM C393
Shear Strength >= 0.400 MPa
>= 58.0 psi
ISO 1922
0.460 MPa
66.7 psi
average; ISO 1922
Thermal Properties Metric English Comments
Thermal Conductivity 0.0330 W/m-K
0.229 BTU-in/hr-ft²-°F
ISO 8301