| Category | Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), Mineral Filled |
| Manufacturer | |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Zytel® HTN 52GM50EF WT001 Polyphthalamide (PPA)
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.70 g/cc | 0.0614 lb/in³ | DAM; ISO 1183 |
| Filler Content | 50 % | 50 % | DAM |
| Linear Mold Shrinkage, Flow | 0.0060 cm/cm <br>@Thickness 2.00 mm |
0.0060 in/in <br>@Thickness 0.0787 in |
DAM; ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.010 cm/cm <br>@Thickness 2.00 mm |
0.010 in/in <br>@Thickness 0.0787 in |
DAM; ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 80.0 MPa <br>@Temperature 23.0 °C |
11600 psi <br>@Temperature 73.4 °F |
DAM; ISO 527 |
| Elongation at Break | 1.3 % <br>@Temperature 23.0 °C |
1.3 % <br>@Temperature 73.4 °F |
DAM; ISO 527 |
| Tensile Modulus | 7.00 GPa <br>@Temperature 23.0 °C |
1020 ksi <br>@Temperature 73.4 °F |
DAM; ISO 527 |
| Flexural Strength | 130 MPa <br>@Temperature 23.0 °C |
18900 psi <br>@Temperature 73.4 °F |
DAM; ISO 178 |
| Flexural Modulus | 6.10 GPa <br>@Temperature 23.0 °C |
885 ksi <br>@Temperature 73.4 °F |
DAM; ISO 178 |
| Charpy Impact, Notched | 0.200 J/cm² <br>@Temperature 23.0 °C |
0.952 ft-lb/in² <br>@Temperature 73.4 °F |
DAM; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 500 µm/m-°C <br>@Temperature -40.0 - 23.0 °C |
278 µin/in-°F <br>@Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
| 500 µm/m-°C <br>@Temperature 160 - 250 °C |
278 µin/in-°F <br>@Temperature 320 - 482 °F |
DAM; ISO 11359-1/-2 | |
| 500 µm/m-°C <br>@Temperature 23.0 - 55.0 °C |
278 µin/in-°F <br>@Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 | |
| 500 µm/m-°C <br>@Temperature 55.0 - 160 °C |
278 µin/in-°F <br>@Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 | |
| CTE, linear, Transverse to Flow | 53.0 µm/m-°C <br>@Temperature -40.0 - 23.0 °C |
29.4 µin/in-°F <br>@Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
| 60.0 µm/m-°C <br>@Temperature 23.0 - 55.0 °C |
33.3 µin/in-°F <br>@Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 | |
| 86.0 µm/m-°C <br>@Temperature 55.0 - 160 °C |
47.8 µin/in-°F <br>@Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 | |
| 100 µm/m-°C <br>@Temperature 160 - 250 °C |
55.6 µin/in-°F <br>@Temperature 320 - 482 °F |
DAM; ISO 11359-1/-2 | |
| Melting Point | 310 °C | 590 °F | 10°C/min, First Heat; DAM; ISO 11357-1/-3 |
| Deflection Temperature at 1.8 MPa (264 psi) | 200 °C | 392 °F | DAM; ISO 75-1/-2 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 325 °C | 617 °F | DAM; Optimum |
| 320 - 330 °C | 608 - 626 °F | DAM | |
| Mold Temperature | 120 - 140 °C | 248 - 284 °F | DAM |
| Drying Temperature | 100 °C | 212 °F | DAM |
| Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | DAM |
| Moisture Content | <= 0.10 % | <= 0.10 % | DAM |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | White Color | DAM |
| Filler | GlassMineral | DAM |
| Forms | Pellets | DAM |
| Material Status | Preliminary Data | DAM |
| Part Marking Code | >PA6T/66-(MD+GF)45< | ISO 11469; DAM |
| >PPA-(MD+GF)45< | SAE J1344; DAM | |
| Processing Method | Injection Molding | DAM |
| Product Category | Glass/Mineral Reinforced Resins | DAM |
| Region Available - Global | Yes | DAM |
| Resin Identification | PA6T/66-(MD+GF)45 | ISO 1043; DAM |
| RoHS Compliance | Contact Manufacturer | DAM |