| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 10% Glass Filled |
| Manufacturer | Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong) |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Cheng Yu Plastic ML3410 PC, 10% Glass Fiber.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
| Linear Mold Shrinkage | 0.0060 - 0.012 cm/cm | 0.0060 - 0.012 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 90 | 90 | ASTM D785 |
| Tensile Strength, Yield | 83.4 MPa | 12100 psi | ASTM D638 |
| Flexural Yield Strength | 127 MPa | 18500 psi | ASTM D790 |
| Izod Impact, Notched | 0.981 J/cm | 1.84 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 146 °C | 295 °F | ASTM D648 |
| Flammability, UL94 | V-2 | V-2 |