Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aremco Corr-Paint™ CP4000 High Temperature Protective Silicone Coating, Metal Oxide Filled

Category Other Engineering Material , Ceramic/Metallic Coating , Polymer , Thermoset , Silicone
Manufacturer Aremco
Trade Name Corr-Paint™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Corr-Paint™ CP4000 High Temperature Protective Silicone Coating, Metal Oxide Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, and offer outstanding resistance to outdoor weathering, UV light, salt spray, chemical corrosion, thermal cycling, and temperatures to 1100 ºF.
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
Solids Content 38.1 %
38.1 %
volume
51.5 %
51.5 %
weight
Volatile Organic Compounds (VOC) Content 125 g/l
125 g/l
Viscosity 400 - 800 cP
400 - 800 cP
Mixed Viscosity
Thickness 25.4 microns
1.00 mil
recommended dry film thickness
66.0 microns
2.60 mil
estimated wet film thickness
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 593 °C
1100 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Processing Temperature 10.0 - 48.9 °C
50.0 - 120 °F
Application Temperature
Dry Time 1.00 - 2.00 hour
1.00 - 2.00 hour
Touch
2.00 - 4.00 hour
2.00 - 4.00 hour
Handling
1.00 - 24.0 hour
1.00 - 24.0 hour
Recoat
Cure Time 45.0 min

@Temperature 249 °C
0.750 hour

@Temperature 480 °F
>1 Hour Air Set Required Prior to Curing
60.0 min

@Temperature 232 °C
1.00 hour

@Temperature 450 °F
>1 Hour Air Set Required Prior to Curing
Shelf Life 6.00 Month

@Temperature 23.0 °C
6.00 Month

@Temperature 73.4 °F
Descriptive Properties Value Comments
Color Flat Black
Dry Film Coverage ft2/gal 611
at 1 mil
Primer Not Required
recommended for exterior applications in which salt fog or moisture are present
Thinner Distilled Water
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved