Thermal Properties Metric English Comments
Glow Wire Test 900 °C

@Thickness 0.750 mm
1650 °F

@Thickness 0.0295 in
Ignition; IEC 60695-2-13
DuPont Performance Polymers Rynite® GW520CS NC010 PET  (Unverified Data**)
Rynite® GW520CS NC010 is a 20% glass fiber reinforced, flame retardant, color stabilized, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Glow Wire Test 900 °C

@Thickness 0.800 mm
1650 °F

@Thickness 0.0315 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance. - Natural: Ixef 1521/0..
Glow Wire Test 900 °C

@Thickness 3.00 mm
1650 °F

@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance. - Natural: Ixef 1521/0..
Glow Wire Test 900 °C

@Thickness 0.400 mm
1650 °F

@Thickness 0.0157 in
DAM; Ignition; IEC 60695-2-13
DuPont Performance Polymers Zytel® 101F BKB009 Nylon 66  (Unverified Data**)
Zytel® 101F BKB009 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Performance Polymers
Glow Wire Test 900 °C

@Thickness 1.50 mm
1650 °F

@Thickness 0.0591 in
GWIT; IEC 60695-2-13
Lanxess Pocan® BF 4232 000000 PBT, 30% Glass Fiber
PBT, 30% glass fiber, injection molding, flame retardantInformation provided by LANXESS.
Glow Wire Test 900 °C

@Thickness 0.400 mm
1650 °F

@Thickness 0.0157 in
GWIT; IEC 60695-2-13
Lanxess Pocan® BF 4232 HR 901510 PBT, 30% Glass Fiber
PBT, 30% glass fiber, injection molding, flame retardant, hydrolysis stabilizedInformation provided by LANXESS.
Glow Wire Test 900 °C

@Thickness 1.00 mm
1650 °F

@Thickness 0.0394 in
GWIT
LATI Latamid 66 H2 G/25-V0CT1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Lat..
Glow Wire Test 900 °C

@Thickness 2.00 mm
1650 °F

@Thickness 0.0787 in
GWIT
LATI Latamid 66 H2 G/25-V0CT1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Lat..
Glow Wire Test 900 °C

@Thickness 3.00 mm
1650 °F

@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA), 50% Glass Fiber
Ixef® 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance.Features: Flame Ret..
Glow Wire Test 900 °C

@Thickness 0.800 mm
1650 °F

@Thickness 0.0315 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA), 50% Glass Fiber
Ixef® 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance.Features: Flame Ret..
Glow Wire Test 900 °C

@Thickness 1.00 mm
1650 °F

@Thickness 0.0394 in
IEC 60695-2-12
Styron CALIBREâ„¢ 301-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-10 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet appli..
Glow Wire Test 900 °C

@Thickness 1.00 mm
1650 °F

@Thickness 0.0394 in
IEC 60695-2-12
Styron CALIBREâ„¢ 301-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-115 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity. The CALIBREâ„¢ 300-10 series products are available in 4 ..
Glow Wire Test 900 °C

@Thickness 1.00 mm
1650 °F

@Thickness 0.0394 in
IEC 60695-2-12
Styron CALIBREâ„¢ 301EP-22 Polycarbonate Resin
Overview: CALIBREâ„¢ 300EP-22 Series are polycarbonate resins that offer exceptional impact resistance, heat distortion resistance and optical clarity for injection molding applications. Their hi..
Glow Wire Test 900 °C

@Thickness 1.60 mm
1650 °F

@Thickness 0.0630 in
ignition temperature; ISO 60695-2-13
Solvay TECHNYL® A 32G1 PA66, DRY
Description: Flame retardant Polyamide 66, unreinforced, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: This flame r..
Glow Wire Test 900 °C

@Thickness 1.00 mm
1650 °F

@Thickness 0.0394 in
IEC 60695-2-12
Styron CALIBREâ„¢ 303-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-10 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet appli..
Glow Wire Test 900 °C

@Thickness 1.00 mm
1650 °F

@Thickness 0.0394 in
IEC 60695-2-12
Styron CALIBREâ„¢ 303-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-115 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity. The CALIBREâ„¢ 300-10 series products are available in 4 ..
Glow Wire Test 900 °C

@Thickness 1.00 mm
1650 °F

@Thickness 0.0394 in
IEC 60695-2-12
Styron CALIBREâ„¢ 303-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-6 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet applic..
Glow Wire Test 900 °C

@Thickness 3.00 mm
1650 °F

@Thickness 0.118 in
GWIT; IEC 60695-2-13
Covestro Makrolon® 2258 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc..
Glow Wire Test 900 °C

@Thickness 0.800 mm
1650 °F

@Thickness 0.0315 in
GWFI; IEC 60695-2-12
Covestro Makrolon® 6255 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Lo..
Glow Wire Test 900 °C

@Thickness 3.00 mm
1650 °F

@Thickness 0.118 in
GWIT; IEC 60695-2-13
Covestro Makrolon® ET3117 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc..
Glow Wire Test 900 °C

@Thickness 3.00 mm
1650 °F

@Thickness 0.118 in
GWIT; IEC 60695-2-13
Covestro Makrolon® ET3127 Polycarbonate
Makrolon® polycarbonate resinMain characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characterist..
Glow Wire Test 900 °C

@Thickness 2.00 mm
1650 °F

@Thickness 0.0787 in
GWIT; IEC 60695
Eurotec® Tecotek® PC30 GR20 GR003 ZG20 PC, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), grey RAL 7035
Information provided by Eurotec®
Glow Wire Test 900 °C

@Thickness 2.00 mm
1650 °F

@Thickness 0.0787 in
GWIT; IEC 60695
Eurotec® Tecotek® PC30 NL TD 700 PC, unfilled, flame retardant - halogen (RoHS compliant), impact modified, natural
Information provided by Eurotec®
Glow Wire Test 900 °C

@Thickness 2.00 mm
1650 °F

@Thickness 0.0787 in
GWIT; IEC 60695
Eurotec® Tecotek® PC44 GR10 GR003 ZG70 PC, 10% glass fiber reinforced, flame retardant - halogen (RoHS compliant), light grey
Information provided by Eurotec®
Glow Wire Test 900 °C

@Thickness 2.00 mm
1650 °F

@Thickness 0.0787 in
GWIT; IEC 60695
Eurotec® Tecotek® PC50 GR10 GR053 FA20 PC, 10% glass fiber reinforced, flame retardant - halogen (RoHS compliant), grey RAL 9002
Information provided by Eurotec®
Glow Wire Test 900 °C

@Thickness 1.00 mm
1650 °F

@Thickness 0.0394 in
DAM; Ignition; IEC 60695-2-13
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont ..
Glow Wire Test 900 °C

@Thickness 3.00 mm
1650 °F

@Thickness 0.118 in
GWIT; IEC 60695-2-13
Lanxess Durethan® AKV 25 F30 000000 Nylon 66, 25% Glass Fiber
PA 66, 25% glass fiber, injection molding, flame retardantInformation provided by LANXESS.