| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.31 g/cc | 0.0473 lb/in³ | |
| 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 | |
| Viscosity | 74660 cP <br>@Shear Rate 5000 1/s,<br> Temperature 270 °C |
74660 cP <br>@Shear Rate 5000 1/s,<br> Temperature 518 °F |
ISO 11403-1 -2 |
| 85140 cP <br>@Shear Rate 5000 1/s,<br> Temperature 260 °C |
85140 cP <br>@Shear Rate 5000 1/s,<br> Temperature 500 °F |
ISO 11403-1 -2 | |
| 98010 cP <br>@Shear Rate 5000 1/s,<br> Temperature 250 °C |
98010 cP <br>@Shear Rate 5000 1/s,<br> Temperature 482 °F |
ISO 11403-1 -2 | |
| 212100 cP <br>@Shear Rate 500 1/s,<br> Temperature 270 °C |
212100 cP <br>@Shear Rate 500 1/s,<br> Temperature 518 °F |
ISO 11403-1 -2 | |
| 242000 cP <br>@Shear Rate 500 1/s,<br> Temperature 260 °C |
242000 cP <br>@Shear Rate 500 1/s,<br> Temperature 500 °F |
ISO 11403-1 -2 | |
| 278600 cP <br>@Shear Rate 500 1/s,<br> Temperature 250 °C |
278600 cP <br>@Shear Rate 500 1/s,<br> Temperature 482 °F |
ISO 11403-1 -2 | |
| Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4 2577 |
| Linear Mold Shrinkage, Transverse | 0.010 cm/cm | 0.010 in/in | ISO 294-4 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 110 MPa | 16000 psi | ISO 527-1/-2 |
| Elongation at Break | 2.7 % | 2.7 % | ISO 527-1/-2 |
| Tensile Modulus | 7.10 GPa | 1030 ksi | ISO 527-1/-2 |
| Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | ISO 179/1eU |
| Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 223 °C | 433 °F | 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 1.8 MPa (264 psi) | 197 °C | 387 °F | ISO 75-1/-2 |
| Flammability, UL94 | V-0 <br>@Thickness 1.50 mm |
V-0 <br>@Thickness 0.0591 in |
IEC 60695-11-10 |
| V-0 <br>@Thickness 0.800 mm |
V-0 <br>@Thickness 0.0315 in |
IEC 60695-11-10 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | IEC 60093 |
| Comparative Tracking Index | 250 V | 250 V | IEC 60112 |
| 175 - 250 V <br>@Thickness 0.750 mm |
175 - 250 V <br>@Thickness 0.0295 in |
UL 746A |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Delivery Form | Pellets | |
| Part Marking Code | >PBT-GF15FR(17)< | ISO 11469 |
| Processing | Injection Moulding | |
| Regional Availability | Asia Pacific | |
| Europe | ||
| Global | ||
| Near East/Africa | ||
| North America | ||
| South and Central America | ||
| UL recognition | UL |