Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Elvax® 770 Ethylene Vinyl Acetate

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Elvax®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF DuPont Elvax® 770 Ethylene Vinyl Acetate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DuPont™ Elvax® 770 is a low BHT anti-oxidant ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications: Elvax® 770 resins can be used for the following applications: molding, compounding and extrusion; hose and tubing; wire and cable; and adhesives, sealants, and wax blends.Information provided by DuPont™
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792-ISO 1183, ASTM D1505
Vinyl Acetate Content 9.5 %
9.5 %
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 98
98
ASTM D2240-ISO 868
Hardness, Shore D 47
47
ASTM D2240-ISO 868
Thermal Properties Metric English Comments
Melting Point 96.0 °C
205 °F
ASTM D3417- ISO 3146
Vicat Softening Point 80.0 °C
176 °F
ASTM D1525, ISO 306
Brittleness Temperature -100 °C
-148 °F
ASTM D746
Ring & Ball Softening Point 227 °C
441 °F
ASTM E28
Descriptive Properties Value Comments
Cloud Point in Paraffin Wax, °C 84
10% Elvax® in fully refined paraffin wax, 146 AMP. Incompatible at temperatures up to 177°C.