| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | <= -100 °C | <= -148 °F | F50, notched specimen; ASTM D 746 |
| NOVA Chemicals Novapol® HB-W555-EC HDPE Blow Molding Resin HB-W555-EC complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biolo.. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D696 |
| NOVA Chemicals Novapol® HB-W747-A HDPE Extrusion Resin Molded Plaque Properties. Features: High molecular weight, excellent ESCR, impact strength, easy processing.Data provided by the manufacturer. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D696 |
| NOVA Chemicals Novapol® HE-Y449-A HDPE Extrusion Resin Features: High ESCR, good toughness, good chemical resistance, good processability.Applications: Pipe coatings, profile extrusions, sheet extrusion for thermoforming, corrugated tubing, conduit.Data.. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D746 |
| NOVA Chemicals Novapol® HE-Y449-AC HDPE Extrusion Resin Medium molecular weight HDPE, Good toughness, Good chemical resistance, Good processabilityApplications: Corrugated tubing, ConduitAdditives: AntioxidantsInformation provided by NOVA Chemicals. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D746 |
| Petromont 4101 High Density Polyethylene Resin Petromont HDPE 4101 is a high density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is primarily used in the extrusion of corrugated pipes for drainage applications, f.. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ISO 974 |
| DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET
(Unverified Data**) Hytrel® DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 49D and contains fine particle size carbon black.In.. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D746 |
| Chevron Phillips HiD® 9412/HiD® 9413 with Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo.. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D746 |
| Chevron Phillips HiD® 99413F with Food Grade Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo.. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D696 |
| NOVA Chemicals Sclair® 35BP HDPE Extrusion Resin, 2.2% Carbon Black Filled
(discontinued **) Features: Excellent ESCR, medium molecular weight, good processability, excellent long term thermal stability, good chemical resistance, excellent UV stability.Applications: Extrusion on to metal pi.. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ASTM D746 |
| A. Schulman LP481 Molding Grade High-Density Polyethylene DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ASTM D746 |
| DuPont Elvax® 150 Ethylene Vinyl Acetate DuPont™ Elvax® 150 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 150 resins can be used for the following applications: molding, compoundin.. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D762 |
| DuPont Elvax® 265 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D762 |
| DuPont Elvax® 460 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ASTM D746 |
| DuPont Elvax® 470 Ethylene Vinyl Acetate DuPont™ Elvax® 470 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Addition: antiblock Applications:Elvax® 470 resins can be used for the following applications: .. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D762 |
| DuPont Elvax® 670 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ASTM D746 |
| DuPont Elvax® 770 Ethylene Vinyl Acetate DuPont™ Elvax® 770 is a low BHT anti-oxidant ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications: Elvax® 770 resins can be used for the following application.. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ASTM D 746 |
| Total 3802 B HDPE, cable, sheet, pipe, injection molding FINATHENE® 3802 B is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low-pressure slurry polymerization process. FINATHENE® 3802 B is a black polyethylene.. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ASTM D 746 |
| Total 3802 Blue MDPE pipe, injection molding FINATHENE® 3802 Blue is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Blue is a blue polyeth.. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ASTM D746 |
| A. Schulman LP642 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 642 is a narrow molecular weight copolymer, high-density polyethylene combining high flow for thin wall articles with excellent toughness. ApplicationApplications of LP 642 include fo.. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D762 |
| DuPont Elvax® 560 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D746 |
| Chevron Phillips Marlex® 9512H - 9513H High Performance Series HDPE Blow Molding Resin Resin Type: linear copolymerCharacteristics: excellent physical properties, medium molecular weight distribution, wide range of processing conditions, good flow for injection blow molding applicatio.. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ASTM D746 |
| DuPont™ Surlyn® 9950 Ionomer Resin, Zinc Surlyn® 9950 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ISO 974 |
| DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl.. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | Compression molded parts prepared according to ASTM D 1928, procedure A.; ASTM D746 |
| Dow DFDC-7525 NT High Density Polyethylene Resin DOW DFDC-7525 NT is produced using UNIPOL™ process technology. It is intended for use in thin wall drip tape and micro-irrigation tube, hose and tube, and profile extrusion applications. Informati.. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | Compression molded parts prepared according to ASTM D 1928, procedure A.; ASTM D746 |
| Dow FLEXOMER™ DFDA-1137 NT 7 Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ DFDA-1137 NT 7 is an ethylene copolymer intended for use in molding and extrusion applications where high flexibility is desired. It is especially useful for flexible hose and tube appli.. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D696 |
| NOVA Chemicals Novapol® HB-W558-A HDPE Extrusion Resin
(discontinued **) Molded Plaque Properties. Features: High molecular weight, excellent impact strength, high rigidity, easy processing.Applications: large part blow molding, large oil drums.Data provided by the manu.. |
|||
| Brittleness Temperature | -100 - -70.0 °C | -148 - -94.0 °F | Average value: -79.3 °C Grade Count:8 |
| Overview of materials for Medium Density Polyethylene (MDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max.. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ASTM D746 |
| A. Schulman LP642 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 642 is a narrow molecular weight copolymer, high-density polyethylene combining high flow for thin wall articles with excellent toughness. ApplicationApplications of LP 642 include fo.. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ASTM D746 |
| DuPont™ Surlyn® 9730 Ionomer Resin, Zinc
(discontinued **) Surlyn® 9730 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ASTM D746 |
| DuPont Elvax® 240 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 240 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 240 resins can be used for the following applications: adhesives, sealants,.. |
|||