Physical Properties Metric English Comments
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Polimeri Europa Clearflex® FG 336 Hexene Copolymer Linear Low Density Polyethylene
Clearflex FG 336 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, slip agent, antiblocking agent and processing aid, suitable for blown film extrusion.Films obtain..
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
SABIC 6821N Linear Low Density Polyethylene for Blown Film
Product Description: 6821N is a fractional melt index hexene copolymer based Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resi..
Melt Flow 0.80 g/10 min

@Load 3.80 kg,
Temperature 230 °C
0.80 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D-1238
Plaskolite West Optix® CA - 1000 E-2 High Impact Acrylic Resin
Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g..
Melt Flow 0.80 g/10 min
0.80 g/10 min
ASTM D1238
Formosa Plastics Formolene® L62608A Film (Hexene Grade) LLDPE  (discontinued **)
Hexene Copolymer (High Antiblock)Applications: Heavy duty shipping sacksHeavy duty shipping sacksInformation provided by Formosa Plastics Corporation, USA.
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Entec Hypel® PEHD.8/.962 HDPE  (discontinued **)
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
NOVA Chemicals Novapol® TF-Y826-D Hexene LLDPE Film Resin
Film Properties. Features: High strength and toughness, excellent puncture resistance, good stiffness and machinability.Applications: Premium trash bags, bags-on-roll.Data provided by the manufactu..
Melt Flow 0.80 g/10 min

@Load 3.80 kg,
Temperature 230 °C
0.80 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Arkema Group Oroglas® DRT Acrylic, Impact Grade  (discontinued **)
For extrusion and injection molding applications. OROGLAS DRT combines good thermal resistance with an excellent impact resistance.Key features : impact resistance: up to 10 times more impact-resis..
Melt Flow 0.80 g/10 min
0.80 g/10 min
Exxon Method
ExxonMobil Iotek® 7010 Zinc Ionomer Molding/Extrusion Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A zinc ionomer with excellent flexibility, abrasion resistance, impact strength and tensile strength. This ionomer has outstanding adhesion to glas..
Melt Flow 0.80 - 1.2 g/10 min

@Load 2.61 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min

@Load 5.75 lb,
Temperature 374 °F
ASTM D1238
LG Chemical SEETEC EF443 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural FilmCSA No. 24937-78-8Information provided by LG Chemical
Melt Flow 0.80 g/10 min
0.80 g/10 min
ISO 1133
Lucite International Diakon® CMH454 Acrylic Polymer
Information provided by Lucite International
Melt Flow 0.80 g/10 min
0.80 g/10 min
ISO 1133
Lucite International Diakon® MH254 Acrylic Bead Polymer, High Transparency
PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte..
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
LyondellBasell Adflexâ„¢ Q 200 F Polyolefin
Description: Adflexâ„¢ Q 200 F fractional melt flow, low modulus thermoplastic olefin (TPO) resin is designed for extrusion applications. It is based on material produced from Basell's propri..
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Borealis Superclean™ LE4244S Polyethylene Insulation Compound, Crosslinkable
Superclean™ LE4244S is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications: Superclean™ LE4244S is intended for insulation of XLPE High Vol..
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
DuPont Elvax® 770 Ethylene Vinyl Acetate
DuPont™ Elvax® 770 is a low BHT anti-oxidant ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications: Elvax® 770 resins can be used for the following application..
Melt Flow 0.80 g/10 min
0.80 g/10 min
ISO 1133
Total FE 8004 LDPE blown film
Radical polyethylene made by high pressure autoclave process. Advised temperature profile : 160 to 200°C.Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former F..
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
A. Schulman PP 1277A-01 Polypropylene High-Impact Polypropylene
DescriptionPolypropylene PP 1277A is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman.
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
Formosa Plastics Formolene® L62608 Film (Hexene Grade) LLDPE
Linear Low Density Polyethylene Hexene Copolymer with High Antiblock for Film Extrusion Formolene® L62608 is a linear low density grade made using gas-phase technology. The resin is designed for he..
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Borealis Borsoft™ SA233CF High Impact Polypropylene Random Heterophasic Copolymer for Blown Film
Borsoft SA233CF is a very soft random heterophasic copolymer, suitable for use on conventional blown film lines with air-coolingBorsoft SA233CF is especially suitable for soft packaging, hygienic fi..
Melt Flow 0.80 g/10 min
0.80 g/10 min
Condition E; ASTM D 1238
Chevron Phillips MarFlex® 5755 LDPE High Clarity, High Impact Film Resin
Resin Type: HomopolymerCharacteristics: High Clarity, Excellent Impact Strength, Medium Slip, High Antiblock, Moderately High Coefficient of Friction, Excellent ProcessabilityApplications:Case Shrin..
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil LLDPE LL 1107X93 Linear Low Density Polyethylene Resin
Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr..
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil LLDPE LL 3201.69 Linear Low Density Polyethylene Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Melt Flow 0.80 g/10 min

@Load 2.16 kg
0.80 g/10 min

@Load 4.76 lb
Dow LDPE 494A Low Density Polyethylene, Film Grade
DOW LDPE 494A resin, is a high strength, general purpose resin used for shipping sack, industrial liner and produce film applications. DOW LDPE 494A resin can be blended with most linear low density..
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Braskem LH 0820/30 AF LLDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Lamination; heavy duty bags; blends with LDPE and HDPE; valvulated heavy duty bags. Information provided by Braske..
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
Bapolene® 108A Low Density Polyethylene Film Extrusion Resin
Bapolene® 108A is an LDPE for blown film. It contains 2500 ppm antiblock additive. This product meets the Food and Drug Administration requirements of 21CFR177.1520.Applications: General purpose p..
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Braskem Green PE SLH0820/30AF Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
Description: SLH0820/30AF is a LLDPE hexene copolymer produced by Braskem. It offers outstanding processability combined with excellent mechanical properties. Very low gel amount. The minimum biobas..
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Phillips 66 COPYLENE® CH008 Polypropylene, Homopolymer, Netting
COPYLENE™ CH008 is a fractional melt flow polypropylene homopolymer resin available in pellet form. Applications: Raffia/Tapes/Strapping; Anti-Corrosion Coating; Geotextile & Agriculture; Nets. Rep..
Melt Flow 0.80 - 1.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
LG Chemical SEETEC SF316 Linear Low Density Polyethylene, Blown Film Grade
Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Additives- Medium slip agent, Medium antiblocking agentApplications: Agricultural & i..
Melt Flow 0.80 - 1.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
LG Chemical SEETEC SF318 Linear Low Density Polyethylene, Blown Film Grade
Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplicati..
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
NOVA Chemicals Novapol® TF-Y826-BP Hexene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Good stiffness and machinability, intended for narrow die gaps, high strength and toughness.Applications: Grocery sacks, boutique bags, frozen food packaging.Data provide..
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
Formosa Plastics Formolene® L62608PA Film (Hexene Grade) LLDPE  (discontinued **)
Linear Low Density Polyethylene Hexene Copolymer with High Antiblock for Film Extrusion Formolene® L62608 is a linear low density grade made using gas-phase technology. The resin is designed for he..
Copyright © lookpolymers.com All Rights Reserved