Eifeler Coatings Technology CrN PVD Coating

Category Ceramic , Nitride , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Eifeler Coatings Technology
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eifeler Coatings Technology CrN PVD Coating.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Key Characteristics: low stress / good adhesion, high toughness and corrosion resistancePrimary Applications: drawing, pressing, bending and stamping of copper and other non-ferrous materials; metal forming; plastic molding; available with in-situ Duplex treatmentInformation provided by Eifeler Coatings Technology
Physical Properties Metric English Comments
Thickness 2.00 - 6.00 microns
0.0787 - 0.236 mil
Mechanical Properties Metric English Comments
Vickers Microhardness 1800 - 2200
1800 - 2200
Coefficient of Friction 0.30 - 0.40
0.30 - 0.40
dry, steel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 600 °C
1110 °F
Descriptive Properties Value Comments
Color silver - gray