Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 80.0 °C | 176 °F | ISO 306/B50 |
Premix Thermoplastics PRE-ELEC® PP 1393 Conductive Thermoplastic Compound PRE-ELEC® PP 1393 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity,.. |
|||
Vicat Softening Point | 80.0 °C | 176 °F | ISO 306 |
Quadrant EPP Cesticolor™ HD 500 Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Vicat Softening Point | 80.0 °C | 176 °F | ISO 306 |
Quadrant EPP Cestilene™ HD 500 R Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Vicat Softening Point | 80.0 °C | 176 °F | 50°C/hr; 50N |
Polimeri Europa EDISTIR PD RK4122H High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,078-06-04-23 UL94 V-2, halogen and antimony free, medium impact polystyrene. This grade features enhanced thermal stabi.. |
|||
Vicat Softening Point | 80.0 °C | 176 °F | |
Eastman Tenite 264-16 CAB Cellulose Acetate Butyrate
(discontinued **) 16% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Vicat Softening Point | 80.0 - 82.0 °C @Load 5.00 kg |
176 - 180 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RH 207/OP Rigid PVC, Antishock Extrusion Medium antishock satined profiles |
|||
Vicat Softening Point | 80.0 - 82.0 °C @Load 5.00 kg |
176 - 180 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RH 210/K1 Rigid PVC, Antishock Extrusion Antishock profiles |
|||
Vicat Softening Point | 80.0 - 82.0 °C @Load 5.00 kg |
176 - 180 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RK 0758 Rigid PVC, Extrusion Lead Free Electric corrugated pipes |
|||
Vicat Softening Point | 80.0 °C | 176 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 65-8347/RD PP-copolymer, with carbon fiber Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & .. |
|||
Vicat Softening Point | 80.0 °C | 176 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 65-8378 PP-copolymer, with carbon fiber Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & .. |
|||
Vicat Softening Point | 80.0 °C | 176 °F | ISO 306 |
Manifattura Cattaneo PE HD Polyethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Vicat Softening Point | 80.0 °C | 176 °F | VST/B/50; ISO 306 |
GEHR Plastics PE-UHMW Polyethylene, Ultra High Molecular Weight The ultra high molecular weight Polyethylene has a high abrasion resistance and a high toughness at the same time. The chemical and the crack resistance are optimized in comparison to the standard P.. |
|||
Vicat Softening Point | 80.0 °C | 176 °F | Rate B; ASTM-D1525 |
Ineos ABS Lustran® ABS 248FC Medical & Food Contact Grade Lustran® ABS 248FC resin is a high-gloss, medium-impact grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of physical properties and has been desi.. |
|||
Vicat Softening Point | 80.0 °C | 176 °F | ASTM D1525 |
Mitsui ADMER® AT2018A PE Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Vicat Softening Point | >= 80.0 °C | >= 176 °F | ASTM D 1525 |
Karina E 830-10/150-Y-ERYB-LMP White PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Vicat Softening Point | >= 80.0 °C | >= 176 °F | ASTM D 1525 |
Karina E 855-10/150-ERYB-PO White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Vicat Softening Point | 80.0 °C @Load 5.00 kg |
176 °F @Load 11.0 lb |
|
LATI Lastilac MR MDT05-01 ABS Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Magnetic detectable filler. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North .. |
|||
Vicat Softening Point | 80.0 °C @Load 5.00 kg |
176 °F @Load 11.0 lb |
|
LATI Latene® EP 22UVH2 MX/25 PP Copolymer, Mineral Reinforced Polypropylene copolymer (PPc) based compound. UV stabilized. Improved thermal stabilization. Special mineral filler. Very good surface appearance. Good elongation.Availability: Africa & Middle East;.. |
|||
Vicat Softening Point | <= 80.0 °C | <= 176 °F | |
Sibur ABS 2020-60 Molding Grade ABS Plastic With anti-static properties for machine building parts. |
|||
Vicat Softening Point | 80.0 °C | 176 °F | ASTM D1525 |
DuPont Bynel® 42E703 Adhesive Resin Bynel® Series 4200 resins are anhydride-modified low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Vicat Softening Point | 80.0 °C | 176 °F | B50 (50°C/h 50N); ISO 306 |
Topas Advanced Polymers TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC) TOPAS® 8007S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma.. |
|||
Vicat Softening Point | 80.0 °C @Load 5.10 kg |
176 °F @Load 11.2 lb |
ASTM D1525 |
Braskem Idealis 500 High Molecular Weight Polyethylene Powder Braskem Idealis 500 is the only High Molecular Weight Polyethylene resin in powder form specially designed for the compression molding process; Applications range from food handling cutting boards a.. |
|||
Vicat Softening Point | 80.0 °C | 176 °F | VST/B/50; ISO 306 |
CENTROPLAST CENTROLEN PE-HD Polyethylene high density This material is a low density, easily machined plastic that can be welded and has good chemical resistance. Applications include apparatus engineering, and machines in the foodstuff industry.Infor.. |
|||
Vicat Softening Point | 80.0 - 118 °C | 176 - 244 °F | Average value: 100 °C Grade Count:88 |
Overview of materials for Cellulose Acetate Butyrate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value.. |
|||
Vicat Softening Point | 80.0 - 104 °C | 176 - 219 °F | Average value: 92.4 °C Grade Count:73 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |
|||
Vicat Softening Point | 80.0 - 112 °C | 176 - 234 °F | Average value: 95.1 °C Grade Count:13 |
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim.. |