| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | <= -100 °C | <= -148 °F | F<sub>50</sub>, notched specimen; ASTM D746 |
| NOVA Chemicals Novapol® HB-W646-U HDPE Blow Molding Resin Features: High molecular weight HDPEExcellent ESCRImpact strengthGood processability Applications: DrumsJerry cansIBCsMarine fuel tanksInformation provided by Nova Chemicals |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D696 |
| NOVA Chemicals Novapol® HD-2100-U MDPE Extrusion Resin Features: Excellent ESCR and toughness, high strength, excellent processability.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provided by the manufacturer. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D696 |
| NOVA Chemicals Novapol® HE-Y449-A HDPE Extrusion Resin Features: High ESCR, good toughness, good chemical resistance, good processability.Applications: Pipe coatings, profile extrusions, sheet extrusion for thermoforming, corrugated tubing, conduit.Data.. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D746 |
| Petromont 3100 High Density Polyethylene Resin Petromont HDPE 3100 is a high density polyethylene resin produced using the UNIPOL® Process. This resin is intended for injection moulding of high performance products such as pails, industrial par.. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D746 |
| Petromont 3101 High Density Polyethylene Resin Petromont HDPE 3101 is a high density polyethylene resin produced using the UNIPOL® Process. This resin is intended for a broad range of injection moulding applications including open-head pails, h.. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ISO 974 |
| DuPont Performance Polymers Hytrel® HTR237BG BK320 TPC-ET
(Unverified Data**) Hytrel® HTR237BG is designed for blow molding or processing techniques requiring high viscosity. It has nominal durometer hardness of 45D, is pigmented black with fine particle size carbon black an.. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ISO 974 |
| DuPont Performance Polymers Hytrel® HTR8223 BK320 TPC-ET
(Unverified Data**) Hytrel® HTR8223 BK320 is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 42D, is pigmented black with fine particle size carbon black, a.. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D746 |
| Chevron Phillips HiD® 9410 HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Wide Range of Processing Conditions, Good Parison Uniformity, Good TrimabilityApplications:Phar.. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D746 |
| Chevron Phillips HiD® 99413F with Food Grade Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo.. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D746 |
| Chevron Phillips HiD® 9404 HDPE Blow Molding Resin
(discontinued **) Resin Type: linear copolymerCharacteristics: medium molecular weight distributions, wide range of processing conditions, low parison sag, good stress crack resistance. Federal specification LP390C .. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D746 |
| Chevron Phillips Marlex® 9506H High Performance Series HDPE Blow Molding Resin
(discontinued **) Resin Type: linear copolymerCharacteristics: superior physical properties, medium molecular weight distribution, wide range of processing conditions, low parison sag, excellent stress crack resistan.. |
|||
| Brittleness Temperature | -100 - -40.0 °C | -148 - -40.0 °F | Average value: -84.7 °C Grade Count:42 |
| Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum .. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D696 |
| NOVA Chemicals Novapol® HD-2100-A MDPE Extrusion Resin
(discontinued **) Features: Excellent ESCR and toughness, high strength, excellent processability.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provided by the manufacturer. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D762 |
| DuPont Elvax® 260 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ASTM D746 |
| DuPont Elvax® 470 Ethylene Vinyl Acetate DuPont™ Elvax® 470 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Addition: antiblock Applications:Elvax® 470 resins can be used for the following applications: .. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ASTM D746 |
| DuPont Elvax® 650Q Ethylene Vinyl Acetate DuPont™ Elvax® 650Q is an ethylene-vinyl acetate copolymer resin for use in industrial applications.Applications:Elvax® 650Q resins can be used for the following applications: molding, compoundin.. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D762 |
| DuPont Elvax® 660 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D762 |
| DuPont Elvax® 670 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ASTM D746 |
| A. Schulman LP642 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 642 is a narrow molecular weight copolymer, high-density polyethylene combining high flow for thin wall articles with excellent toughness. ApplicationApplications of LP 642 include fo.. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ASTM D746 |
| A. Schulman LP642 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 642 is a narrow molecular weight copolymer, high-density polyethylene combining high flow for thin wall articles with excellent toughness. ApplicationApplications of LP 642 include fo.. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ASTM D 746 |
| Total 3802 YCF MDPE pipe grade FINATHENE® 3802 Y CF is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Y CF is a yellow cadmi.. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ASTM D746 |
| A. Schulman LP481 Molding Grade High-Density Polyethylene DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ASTM D746 |
| DuPont™ Surlyn® 9950 Ionomer Resin, Zinc Surlyn® 9950 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ISO 974 |
| DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl.. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | Compression molded parts prepared according to ASTM D 1928, procedure A.; ASTM D746 |
| Dow FINGERPRINT™ DFDA-7510 NT Linear Low Density Polyethylene Resin FINGERPRINT™ DFDA-7510 NT resin is produced using UNIPOL™ process technology. It is intended for use in micro irrigation tube, durable hose and tube, profile extrusion, and injection molded fitti.. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | Compression molded parts prepared according to ASTM D 1928, procedure A.; ASTM D746 |
| Dow DNDB-7441 NT 7 Linear Low Density Polyethylene Resin DOW DNDB-7441 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in hose and tube applications. It also has utility in gasketing, spiral wound hose, and corrugated hose .. |
|||
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D696 |
| NOVA Chemicals Sclair® 35BPM MDPE Extrusion Resin, 2.2% Carbon Black Filled
(discontinued **) Features: Excellent ESCR, medium molecular weight, good processability, excellent long term thermal stability, good chemical resistance, excellent UV stability.Applications: Extrusion on to metal pi.. |
|||
| Brittleness Temperature | -100 - -70.0 °C | -148 - -94.0 °F | Average value: -79.3 °C Grade Count:8 |
| Overview of materials for Medium Density Polyethylene (MDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max.. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ASTM D746 |
| A. Schulman LP642 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 642 is a narrow molecular weight copolymer, high-density polyethylene combining high flow for thin wall articles with excellent toughness. ApplicationApplications of LP 642 include fo.. |
|||
| Brittleness Temperature | -100 °C | -148 °F | ASTM D746 |
| DuPont Elvax® 760Q Ethylene Vinyl Acetate DuPont™ Elvax® 760W is a low BHT anti-oxidant ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications: Elvax® 760Q resins can be used for the following applicati.. |
|||