| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.52 g/cc | 0.0549 lb/in³ | dry; ISO 1183 |
| Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | Sim. To ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | Sim. To ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 55.0 MPa | 7980 psi | dry; ISO 527-1/-2 |
| Elongation at Break | 2.0 % | 2.0 % | dry; ISO 527-1/-2 |
| Tensile Modulus | 5.10 GPa | 740 ksi | dry; ISO 527-1/-2 |
| Izod Impact Resistance | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 180/1A |
| Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 48.0 µm/m-°C | 26.7 µin/in-°F | dry; ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 48.0 µm/m-°C | 26.7 µin/in-°F | dry; ISO 11359-1/-2 |
| Thermal Conductivity | 0.500 W/m-K | 3.47 BTU-in/hr-ft²-°F | through plane; ASTM E1461 |
| 1.00 W/m-K | 6.94 BTU-in/hr-ft²-°F | in plane; ASTM E1461 | |
| UL RTI, Electrical | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL746B |
| Flammability, UL94 | V-0 @Thickness 1.50 mm |
V-0 @Thickness 0.0591 in |
dry; IEC 60695-11-10 |
| V-0 @Thickness 0.750 mm |
V-0 @Thickness 0.0295 in |
dry; IEC 60695-11-10 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | dry; IEC 60093 |
| Dielectric Strength | 30.0 kV/mm | 762 kV/in | dry; IEC 60243-1 |