| Category | Polymer , Thermoplastic , Nylon , Nylon 6/66 |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Novamid® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DSM Novamid® 2430A-1 PA666.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | dry; ISO 1183 |
| Moisture Absorption | 3.50 % | 3.50 % | Sim. To ISO 62 |
| Viscosity | 90000 cP <br>@Shear Rate 10000 1/s,<br> Temperature 240 °C |
90000 cP <br>@Shear Rate 10000 1/s,<br> Temperature 464 °F |
|
| 90000 cP <br>@Shear Rate 10000 1/s,<br> Temperature 260 °C |
90000 cP <br>@Shear Rate 10000 1/s,<br> Temperature 500 °F |
||
| 90000 cP <br>@Shear Rate 10000 1/s,<br> Temperature 280 °C |
90000 cP <br>@Shear Rate 10000 1/s,<br> Temperature 536 °F |
||
| 2.00e+6 cP <br>@Shear Rate 0.100 1/s,<br> Temperature 280 °C |
2.00e+6 cP <br>@Shear Rate 0.100 1/s,<br> Temperature 536 °F |
||
| 3.00e+6 cP <br>@Shear Rate 0.100 1/s,<br> Temperature 260 °C |
3.00e+6 cP <br>@Shear Rate 0.100 1/s,<br> Temperature 500 °F |
||
| 5.00e+6 cP <br>@Shear Rate 0.100 1/s,<br> Temperature 240 °C |
5.00e+6 cP <br>@Shear Rate 0.100 1/s,<br> Temperature 464 °F |
||
| Viscosity Test | 246 cm³/g | 246 cm³/g | Viscosity Number; ISO 307, 1157, 1628 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 193 °C | 379 °F | 10°C/min; ISO 11357-1/-3 |
| Flammability, UL94 | HB <br>@Thickness 1.50 mm |
HB <br>@Thickness 0.0591 in |
dry; IEC 60695-11-10 |
| HB <br>@Thickness 0.800 mm |
HB <br>@Thickness 0.0315 in |
dry; IEC 60695-11-10 |