Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Stanyl® TW241F12 (DAM) Nylon 46 60% Glass Reinforced, Heat Stabilized, High Flow (North America)

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Glass Fiber Reinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF DSM Stanyl® TW241F12 (DAM) Nylon 46 60% Glass Reinforced, Heat Stabilized, High Flow (North America).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by DSM Engineering Plastics.
Physical Properties Metric English Comments
Density 1.76 g/cc
0.0636 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 255 MPa
37000 psi
ISO 527-1/-2
Elongation at Break 2.0 %
2.0 %
ISO 527-1/-2
Tensile Modulus 20.0 GPa
2900 ksi
ISO 527-1/-2
Charpy Impact Unnotched 9.00 J/cm²
42.8 ft-lb/in²
ISO 179/1eU
8.00 J/cm²

@Temperature -30.0 °C
38.1 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.90 J/cm²
9.04 ft-lb/in²
ISO 179/1eU
1.90 J/cm²

@Temperature -30.0 °C
9.04 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C

@Temperature 20.0 °C
11.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
Melting Point 295 °C
563 °F
ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 290 °C
554 °F
ISO 75-1/-2