Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Akulon® Ultraflow™ K-FHG0 Nylon 6-50% Glass Reinforced (European Grade) (Cond)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 50% Glass Fiber Filled
Manufacturer DSM Engineering Plastics
Trade Name Akulon® Ultraflow™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Akulon® Ultraflow™ K-FHG0 Nylon 6-50% Glass Reinforced (European Grade) (Cond).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier film, stock shapes, convoluted tubes, and monofilament. Akulon XP is a high-productivity, high-performance PA6 grade for film extrusion processes. Medium viscosity, unreinforced or reinforced Akulon grades are used for various injection molding and blow molding applications. Akulon® Ultraflow® is a high-productivity, high-performance PA6 family for molding processes.Key applications for Akulon: Automotive: Intake manifold, Engine, Powertrain, Airbag containers, Exterior trim, Interior trim, Electrical components and connectorsConsumer durables: Power tools, Lawn and garden tools, Small appliances, Sports and leisure equipment, Furniture, Industrial Goods, TransportationE&E: Low voltage switch gear/power distribution, Lighting, Power connectorsFilm: Specialty and barrier filmsInformation provided by DSM.
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
(DAM); ISO 1183
Water Absorption 4.5 %
4.5 %
DAM; Sim. to ISO 62
Moisture Absorption at Equilibrium 1.4 %
1.4 %
Humidity Absorption (DAM); Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
DAM; ISO 294-4
0.0090 cm/cm
0.0090 in/in
DAM; ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 160 MPa
23200 psi
ISO 527-1/-2
Elongation at Break 5.0 %
5.0 %
ISO 527-1/-2
Tensile Modulus 11.0 GPa
1600 ksi
ISO 527-1/-2
Charpy Impact Unnotched 8.50 J/cm²

@Temperature -30.0 °C
40.5 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
10.0 J/cm²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min (DAM); ISO 11357-1/-3
Electrical Properties Metric English Comments
Dielectric Constant 4.5

@Frequency 1e+6 Hz
4.5

@Frequency 1e+6 Hz
IEC 60250
14

@Frequency 100 Hz
14

@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.12

@Frequency 1e+6 Hz
0.12

@Frequency 1e+6 Hz
IEC 60250
0.30

@Frequency 100 Hz
0.30

@Frequency 100 Hz
IEC 60250
Descriptive Properties Value Comments
Heat stabilized or stable to heat Yes
Injection molding Yes
With Fillers Yes
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved