| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Akulon® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | DSM Akulon® S245-C PA66.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | dry; ISO 1183 |
| Water Absorption | 9.0 % | 9.0 % | Sim. To ISO 62 |
| Moisture Absorption | 2.50 % | 2.50 % | Sim. To ISO 62 |
| Viscosity Test | 330 cm³/g | 330 cm³/g | Viscosity Number; ISO 307, 1157, 1628 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact Unnotched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
dry; ISO 179/1eU |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
dry; ISO 179/1eU |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | dry; ISO 11359-1/-2 |
| Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | dry; IEC 60093 |
| Dielectric Constant | 3.3 @Frequency 1.00e+6 Hz |
3.3 @Frequency 1.00e+6 Hz |
dry; IEC 60250 |
| 3.6 @Frequency 100 Hz |
3.6 @Frequency 100 Hz |
dry; IEC 60250 | |
| Dielectric Strength | 25.0 kV/mm | 635 kV/in | dry; IEC 60243-1 |
| Dissipation Factor | 0.0090 @Frequency 100 Hz |
0.0090 @Frequency 100 Hz |
dry; IEC 60250 |
| 0.022 @Frequency 1.00e+6 Hz |
0.022 @Frequency 1.00e+6 Hz |
dry; IEC 60250 |