Kazanorgsintez PE2NT74-15 High Density Polyethylene for Blow Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Kazanorgsintez
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kazanorgsintez PE2NT74-15 High Density Polyethylene for Blow Molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Production Method: Gaseous-phase method. Application: Compositions are intended for goods produced by injection molding method.Information Provided by Kazanorgsintez
Physical Properties Metric English Comments
Density 0.946 - 0.953 g/cc

@Temperature 23.0 °C
0.0342 - 0.0344 lb/in³

@Temperature 73.4 °F
0.949 - 0.955 g/cc

@Temperature 20.0 °C
0.0343 - 0.0345 lb/in³

@Temperature 68.0 °F
Environmental Stress Crack Resistance >= 30 hour
>= 30 hour
Melt Flow 1.5 - 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.5 - 2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 26.0 MPa
>= 3770 psi
Elongation at Break >= 750 %
>= 750 %
Tear Strength Test >= 30
>= 30
MPa