Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
1.02 g/cc @Temperature 260 °C |
0.0368 lb/in³ @Temperature 500 °F |
Melt | |
Water Absorption | 0.50 % | 0.50 % | Similar to ISO 62 |
Moisture Absorption at Equilibrium | 0.20 % | 0.20 % | Similar to ISO 62 |
Melt Flow | 18 g/10 min @Load 5.00 kg, Temperature 260 °C |
18 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 60.0 MPa | 8700 psi | ISO 527-1/-2 |
Elongation at Break | >= 50 % | >= 50 % | Nominal; ISO 527-1/-2 |
Elongation at Yield | 5.0 % | 5.0 % | ISO 527-1/-2 |
Tensile Modulus | 2.20 GPa | 319 ksi | ISO 527-1/-2 |
Charpy Impact Unnotched | NB | NB | ISO 179/1eU |
NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
ISO 179/1eU | |
Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | ISO 179/1eA |
4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA | |
Impact | 3800 | 3800 | Puncture - maximum force (N); ISO 6603-2 |
5000 @Temperature -30.0 °C |
5000 @Temperature -22.0 °F |
Puncture - maximum force (N); ISO 6603-2 | |
Puncture Energy | 47.0 J | 34.7 ft-lb | ISO 6603-2 |
58.0 J @Temperature -30.0 °C |
42.8 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
Specific Heat Capacity | 1.82 J/g-°C | 0.435 BTU/lb-°F | Melt |
Thermal Conductivity | 0.179 W/m-K | 1.24 BTU-in/hr-ft²-°F | Melt |
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ISO 75-1/-2 |
Deflection Temperature at 1.8 MPa (264 psi) | 85.0 °C | 185 °F | ISO 75-1/-2 |
Flammability, UL94 | HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
IEC 60695-11-10 |
Oxygen Index | 21 % | 21 % | ISO 4589-1/-2 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | IEC 60093 |
Dielectric Constant | 3.0 @Frequency 1.00e+6 Hz |
3.0 @Frequency 1.00e+6 Hz |
IEC 60250 |
3.2 @Frequency 100 Hz |
3.2 @Frequency 100 Hz |
IEC 60250 | |
Dielectric Strength | 30.0 kV/mm | 762 kV/in | IEC 60243-1 |
Dissipation Factor | 0.00070 @Frequency 100 Hz |
0.00070 @Frequency 100 Hz |
IEC 60250 |
0.0045 @Frequency 1.00e+6 Hz |
0.0045 @Frequency 1.00e+6 Hz |
IEC 60250 | |
Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
260 °C | 500 °F | Injection Molding; ISO 294 | |
Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
70.0 °C | 158 °F | Injection Molding; ISO 10724 | |
Ejection Temperature | 170 °C | 338 °F | |
Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
Descriptive Properties | Value | Comments |
---|---|---|
Availability | Asia Pacific | |
Europe | ||
India | ||
Near East/Africa | ||
North America | ||
South and Central America | ||
Eff. thermal diffusivity (m²/s) | 9.64E-08 | |
Feature | Release agent | |
Form | Pellets | |
Process | Injection Molding |