| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 102 °C @Load 1.00 kg |
216 °F @Load 2.20 lb |
120°C/min; ASTM D1525 |
| Kingfa FRABS V-0 Flame Retardant ABS Features:UL 94 V-0 @ 1.5-3.0mmHigh toughnessFor extrusion moldingApplications:PlateElectric and electronic cabinetPCB boardInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
| Vicat Softening Point | 102 °C @Load 0.999 kg |
216 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTADIENE 1030 V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, good impact resistance, high gloss, good light resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 102 °C @Load 0.999 kg |
216 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTADIENE 1030 V0/Ex Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high impact resistance, high gloss, good light resistance, for extrusionInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 102 °C @Load 0.999 kg |
216 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTADIENE 1640 AS Acrylonitrile Butadiene Styrene General purpose ABSGood impact resistance, high melt flow rate, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 102 °C @Load 5.00 kg |
216 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTADIENE 2020 MT Acrylonitrile Butadiene Styrene ABSMedium heat resistance, good impact resistance, good melt flow rate, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 102 °C @Load 5.00 kg |
216 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTADIENE 2506 Acrylonitrile Butadiene Styrene ABS for sheet and profile extrusionHigh impact resistance, excellent heat resistance, excellent dimensional stability and processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 102 °C @Load 5.00 kg |
216 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTADIENE 3015 MT Acrylonitrile Butadiene Styrene ABSMedium thermal resistance, high impact resistance at low temperature, good melt flow rate, high gloss, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 102 °C @Load 1.02 kg |
216 °F @Load 2.25 lb |
120°C/hr; ISO 306 |
| Cossa Polimeri ESTALUX 5513 Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 102 °C @Load 1.02 kg |
216 °F @Load 2.25 lb |
120°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTALUX 9206 A Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 102 °C @Load 1.02 kg |
216 °F @Load 2.25 lb |
120°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTALUX 9206 Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMABiomedical grade in line with US pharmacopeia class VI USP and European pharmacopeia cap. 3.2.2Information.. |
|||
| Vicat Softening Point | 102 °C @Load 5.00 kg |
216 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTASAN SAN 2000 Styrene Acrylonitrile General purpose SANGood chemical resistance, excellent dimensional stabilityInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 102 °C @Load 5.00 kg |
216 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTASAN SAN 3000 Styrene Acrylonitrile High melt flow rate, good chemical resistance, excellent dimensional stabilityInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 102 °C @Load 5.10 kg |
216 °F @Load 11.2 lb |
50°C/h; ISO 306 |
| Covestro Bayblend® FR3005 HG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
| Vicat Softening Point | 102 °C @Load 5.10 kg |
216 °F @Load 11.2 lb |
120°C/h; ISO 306 |
| Covestro Bayblend® FR3012 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
| Vicat Softening Point | 102 °C @Load 5.00 kg |
216 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Kibisan® PN-117 SAN Injection Molding |
|||
| Vicat Softening Point | 102 °C @Load 5.00 kg |
216 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Kibisan® PN-117C SAN High Clarity |
|||
| Vicat Softening Point | 102 °C @Load 5.00 kg |
216 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
| Chi Mei Polylac® PA-709S ABS - Extrusion Super Impact Extrusion |
|||
| Vicat Softening Point | 102 °C @Load 1.00 kg |
216 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-746 ABS - High Flow High flow, medium impact |
|||
| Vicat Softening Point | 102 °C @Load 5.00 kg |
216 °F @Load 11.0 lb |
50°C/hr; ASTM D1525 |
| Diamond Polymers Centrex® 925 Injection Molding Grade Centrex 925 resin is a soft-flow, high-gloss, molding grade of Polycarbonate / ASA (acrylonitrile-styrene-acrylate) blend. It is an injection molding grade with a good balance of physical properties.. |
|||
| Vicat Softening Point | 102 °C @Load 5.00 kg |
216 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Cossa Polimeri ESTABLEND PA 2500 ABS / Nylon 6 Blend ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.Easy processing, high surface quality, high chemical resistance, good heat resistanceInformation provided by Cossa Polimeri.. |
|||
| Vicat Softening Point | 102 °C @Load 5.00 kg |
216 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
| Chi Mei Polylac® PA-707 ABS High gloss, high rigid |
|||
| Vicat Softening Point | 102 °C @Load 1.00 kg |
216 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-727 ABS Electro-plating |
|||
| Vicat Softening Point | 102 °C @Load 1.00 kg |
216 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-746H ABS - High Flow Super high flow, medium impact |
|||
| Vicat Softening Point | 102 °C @Load 5.00 kg |
216 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
| Chi Mei Polylac® PA-747S ABS - Extrusion High Impact Extrusion |
|||
| Vicat Softening Point | 102 °C @Load 1.00 kg |
216 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-756H ABS - High Flow Super high flow |
|||
| Vicat Softening Point | 102 °C @Load 1.00 kg |
216 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-756S ABS - High Flow Super high flow, medium impact |
|||
| Vicat Softening Point | 102 °C @Load 1.00 kg |
216 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-758R ABS - Transparent Transparent, Chemical Resistant |
|||
| Vicat Softening Point | 102 °C @Load 1.00 kg |
216 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
| Chi Mei Polyrex® PG-80 Polystyrene High strength |
|||
| Vicat Softening Point | 102 °C @Load 1.00 kg |
216 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polyrex® PH-888H Polystyrene - High Impact High FDI; high heat |
|||