Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont™ Nucrel® 30705 Ethylene Acrylic Acid

Category Polymer , Thermoplastic , Ethylene Acrylic Acid
Manufacturer DuPont
Trade Name Nucrel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Nucrel® 30705 Ethylene Acrylic Acid.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Nucrel® 30705 is an ethylene-acrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethylene resin. This resin may also be used in conventional blown and cast film extrusion and coextrusion equipment. Uses: Adhesives Packaging Sealants Composition: 7 % By Weight Acrylic Acid comonomer content Nucrel® 30705 conforms to the U.S. Code of Federal Regulations, Title 21, Paragraph 177.1310, covering its use as a food contact surface subject to the extractives limitations on the finished food contact article as described in the regulation.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792, ISO 1183
Melt Flow 5.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Thermal Properties Metric English Comments
Melting Point 89.0 °C
192 °F
Freezing Point; ASTM D3418, ISO 3146
107 °C
225 °F
ASTM D3418, ISO 3146
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525, ISO 306
Processing Properties Metric English Comments
Processing Temperature <= 310 °C
<= 590 °F
Feed Temperature 135 °C
275 °F
Blown Film Coextrusion
185 °C
365 °F
Extrusion Coating
Zone 2 160 °C
320 °F
Blown Film Coextrusion
235 °C
455 °F
Extrusion Coating
Zone 3 185 °C
365 °F
Blown Film Coextrusion
285 °C
545 °F
Extrusion Coating
Zone 4 185 °C
365 °F
Blown Film Coextrusion
300 °C
572 °F
Extrusion Coating
Zone 5 185 °C
365 °F
Blown Film Coextrusion
300 °C
572 °F
Extrusion Coating
Adapter Temperature 185 °C
365 °F
Blown Film Coextrusion
300 °C
572 °F
Extrusion Coating
Die Temperature 185 °C
365 °F
Blown Film Coextrusion
300 °C
572 °F
Extrusion Coating
Melt Temperature 160 - 285 °C
320 - 545 °F
Extrusion Coating
Users viewing this material also viewed the following: