Thermal Properties Metric English Comments
Vicat Softening Point 102 °C
<br>@Load 1.00 kg
216 °F
<br>@Load 2.20 lb
120°C/min; ASTM D1525
Kingfa FRABS V-0 Flame Retardant ABS
Features:UL 94 V-0 @ 1.5-3.0mmHigh toughnessFor extrusion moldingApplications:PlateElectric and electronic cabinetPCB boardInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Vicat Softening Point 102 °C
<br>@Load 0.999 kg
216 °F
<br>@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 1030 V0 Flame Retardant ABS
Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, good impact resistance, high gloss, good light resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 102 °C
<br>@Load 0.999 kg
216 °F
<br>@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 1030 V0/Ex Flame Retardant ABS
Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high impact resistance, high gloss, good light resistance, for extrusionInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 102 °C
<br>@Load 0.999 kg
216 °F
<br>@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 1640 AS Acrylonitrile Butadiene Styrene
General purpose ABSGood impact resistance, high melt flow rate, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 102 °C
<br>@Load 5.00 kg
216 °F
<br>@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 2020 MT Acrylonitrile Butadiene Styrene
ABSMedium heat resistance, good impact resistance, good melt flow rate, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 102 °C
<br>@Load 5.00 kg
216 °F
<br>@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 2506 Acrylonitrile Butadiene Styrene
ABS for sheet and profile extrusionHigh impact resistance, excellent heat resistance, excellent dimensional stability and processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 102 °C
<br>@Load 5.00 kg
216 °F
<br>@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 3015 MT Acrylonitrile Butadiene Styrene
ABSMedium thermal resistance, high impact resistance at low temperature, good melt flow rate, high gloss, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 102 °C
<br>@Load 1.02 kg
216 °F
<br>@Load 2.25 lb
120°C/hr; ISO 306
Cossa Polimeri ESTALUX 5513 Methyl Methacrylate Acrylonitrile Butadiene Styrene
Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 102 °C
<br>@Load 1.02 kg
216 °F
<br>@Load 2.25 lb
120°C/hr; ASTM D 1525
Cossa Polimeri ESTALUX 9206 A Methyl Methacrylate Acrylonitrile Butadiene Styrene
Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 102 °C
<br>@Load 1.02 kg
216 °F
<br>@Load 2.25 lb
120°C/hr; ASTM D 1525
Cossa Polimeri ESTALUX 9206 Methyl Methacrylate Acrylonitrile Butadiene Styrene
Plastic blend that combines impact properties of ABS with the excellent transparency of PMMABiomedical grade in line with US pharmacopeia class VI USP and European pharmacopeia cap. 3.2.2Information..
Vicat Softening Point 102 °C
<br>@Load 5.00 kg
216 °F
<br>@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTASAN SAN 2000 Styrene Acrylonitrile
General purpose SANGood chemical resistance, excellent dimensional stabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 102 °C
<br>@Load 5.00 kg
216 °F
<br>@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTASAN SAN 3000 Styrene Acrylonitrile
High melt flow rate, good chemical resistance, excellent dimensional stabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 102 °C
<br>@Load 5.10 kg
216 °F
<br>@Load 11.2 lb
50°C/h; ISO 306
Covestro Bayblend® FR3005 HG PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Vicat Softening Point 102 °C
<br>@Load 5.10 kg
216 °F
<br>@Load 11.2 lb
120°C/h; ISO 306
Covestro Bayblend® FR3012 PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Vicat Softening Point 102 °C
<br>@Load 5.00 kg
216 °F
<br>@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Kibisan® PN-117 SAN
Injection Molding
Vicat Softening Point 102 °C
<br>@Load 5.00 kg
216 °F
<br>@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Kibisan® PN-117C SAN
High Clarity
Vicat Softening Point 102 °C
<br>@Load 5.00 kg
216 °F
<br>@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-709S ABS - Extrusion
Super Impact Extrusion
Vicat Softening Point 102 °C
<br>@Load 1.00 kg
216 °F
<br>@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-746 ABS - High Flow
High flow, medium impact
Vicat Softening Point 102 °C
<br>@Load 5.00 kg
216 °F
<br>@Load 11.0 lb
50°C/hr; ASTM D1525
Diamond Polymers Centrex® 925 Injection Molding Grade
Centrex 925 resin is a soft-flow, high-gloss, molding grade of Polycarbonate / ASA (acrylonitrile-styrene-acrylate) blend. It is an injection molding grade with a good balance of physical properties..
Vicat Softening Point 102 °C
<br>@Load 5.00 kg
216 °F
<br>@Load 11.0 lb
50°C/hr; ISO 306
Cossa Polimeri ESTABLEND PA 2500 ABS / Nylon 6 Blend
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.Easy processing, high surface quality, high chemical resistance, good heat resistanceInformation provided by Cossa Polimeri..
Vicat Softening Point 102 °C
<br>@Load 5.00 kg
216 °F
<br>@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-707 ABS
High gloss, high rigid
Vicat Softening Point 102 °C
<br>@Load 1.00 kg
216 °F
<br>@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-727 ABS
Electro-plating
Vicat Softening Point 102 °C
<br>@Load 1.00 kg
216 °F
<br>@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-746H ABS - High Flow
Super high flow, medium impact
Vicat Softening Point 102 °C
<br>@Load 5.00 kg
216 °F
<br>@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-747S ABS - Extrusion
High Impact Extrusion
Vicat Softening Point 102 °C
<br>@Load 1.00 kg
216 °F
<br>@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-756H ABS - High Flow
Super high flow
Vicat Softening Point 102 °C
<br>@Load 1.00 kg
216 °F
<br>@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-756S ABS - High Flow
Super high flow, medium impact
Vicat Softening Point 102 °C
<br>@Load 1.00 kg
216 °F
<br>@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-758R ABS - Transparent
Transparent, Chemical Resistant
Vicat Softening Point 102 °C
<br>@Load 1.00 kg
216 °F
<br>@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polyrex® PG-80 Polystyrene
High strength
Vicat Softening Point 102 °C
<br>@Load 1.00 kg
216 °F
<br>@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polyrex® PH-888H Polystyrene - High Impact
High FDI; high heat