Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CP-Polymer-Technik Wellamid® 6000 MRGV 25/15 HWUVCP 25% Mineral and 15% Glass Fiber Nylon 6, UV Stabilized, Heat Stabilized, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer CP-Polymer-Technik GmbH & Co.
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CP-Polymer-Technik Wellamid® 6000 MRGV 25/15 HWUVCP 25% Mineral and 15% Glass Fiber Nylon 6, UV Stabilized, Heat Stabilized, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by CP-Polymer-Technik GmbH & Co. KG
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 1.5 - 2.0 %
1.5 - 2.0 %
23°C/50%RH, Starting when dry; DIN 53495
Linear Mold Shrinkage 0.0050 cm/cm

@Thickness 4.00 mm
0.0050 in/in

@Thickness 0.157 in
Linear Mold Shrinkage, Transverse 0.0070 cm/cm

@Thickness 4.00 mm
0.0070 in/in

@Thickness 0.157 in
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
5 mm/min; ISO 527
Elongation at Break 7.0 %
7.0 %
5 mm/min; ISO 527
Tensile Modulus 5.20 GPa
754 ksi
ISO 527
Charpy Impact Unnotched 8.00 J/cm²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 1.60 J/cm²

@Temperature 23.0 °C
7.61 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
Kofler
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 93
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
ISO 3915
Dielectric Constant 6.0

@Frequency 1e+6 Hz
6.0

@Frequency 1e+6 Hz
IEC 250
Dielectric Strength 35.0 kV/mm
889 kV/in
IEC 243-1
Dielectric Loss Index 0.20
0.20
At 1 MHz; IEC 250
Processing Properties Metric English Comments
Melt Temperature 260 - 290 °C
500 - 554 °F
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Descriptive Properties Value Comments
Back Pressure Low
Holding Pressure High
Injection Speed High
Screw Speed High
Users viewing this material also viewed the following: