Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Petrothene® GA837091 Medium Density Polyethylene
(Unverified Data**) ApplicationsPETROTHENE GA 837-091 is a broad molecular weight, medium density resin designed for use as a base resin in wire and cable jacketing. An antioxidant has been added to ensure thermal st.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746A |
Solvay Specialty Polymers Halar® 500LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Brittleness Temperature | -76.0 - 20.0 °C | -105 - 68.0 °F | Average value: -69.6 °C Grade Count:15 |
Overview of materials for ECTFE Fluoropolymer This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Alathon® L5440 High Density Polyethylene ApplicationsALATHON L 5440 is designed for high shear machines. It exhibits excellent color, low odor and excellent processing stability. Typical applications include general purpose, household ch.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Alathon® M4612 High Density Polyethylene ApplicationsALATHON M 4612 is a copolymer that provides outstanding ESCR and low temperature impact strength. Typical applications include food containers, seat hinges, tube headers.Regulatory Stat.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Alathon® M6080WC High Density Polyethylene ApplicationsALATHON M 6080WC is a natural, high density, polyethylene homopolymer resin with a narrow molecular weight distribution formulated for use as primary insulation for coaxial and control c.. |
|||
Brittleness Temperature | -76.0 °C | -105 °F | ASTM D746 |
LyondellBasell Microthene® F FA70900 High Density Polyethylene General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<SUB>50</SUB>; ASTM D746 |
LyondellBasell Petrothene® GA564189 Linear Low Density Polyethylene, Injection Molding Grade PETROTHENE GA564189 exhibits good stiffness and low temperature toughness. Typical applications include trash cans, industrial containers, housewares and toys. Regulatory Status: GA564189 meets the .. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Petrothene® LB5604 High Density Polyethylene ApplicationsThe PETROTHENE LB 5604 series of polyethylene resins exhibits good stiffness and environmental stress cracking resistance. Typical applications include household chemical and person car.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Petrothene® LR732011 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Typical applications include bottles for bleac.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Petrothene® LR734001 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<SUB>50</SUB>; ASTM D746 |
LyondellBasell Petrothene® NA149000 Low Density Polyethylene, Blow Molding Grade PETROTHENE NA149000 resin exhibits an excellent balance of toughness and softness, with excellent dimensional stability. Typical applications include housewares, toys, containers and novelty items. .. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<SUB>50</SUB>; ASTM D746 |
LyondellBasell Petrothene® NA149000 Low Density Polyethylene, Sheet Extrusion Grade PETROTHENE NA149000 resin exhibits an excellent balance of toughness and softness, with excellent dimensional stability. Typical applications include housewares, toys, containers and novelty items. .. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Petrothene® NA324009 Low Density Polyethylene (Blow Molding Applications) ApplicationsPETROTHENE NA 324-009 is a low density homopolymer resin intended for blow molding applications. NA 324-009 provides good clarity, toughness and processability. Typical applications in.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | molding; ASTM D746 |
LyondellBasell Petrothene® NA967000 Low Density Polyethylene, Film Extrusion Grade Petrothene NA967000 is a low density polyethylene resin designed for blown film, general purpose and industrial packaging applications. NA967000 exhibits good processing characteristics and impact s.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
LyondellBasell Ultrathene® UE672006 Ethylene Vinyl Acetate Copolymer, Film Grade Ultrathene UE672 is an EVA copolymer with excellent impact strength, heat sealability, good toughness and flexibility. Applications may include flexible packaging films for food and healthcare, as w.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
LyondellBasell Ultrathene® UE672317 Ethylene Vinyl Acetate Copolymer, Film Grade Ultrathene UE672 is an EVA copolymer with excellent impact strength, heat sealability, good toughness and flexibility. Applications may include flexible packaging films for food and healthcare, as w.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D 746 |
LyondellBasell Petrothene® LM600700 High Density Polyethylene (Blow Molding Grade) ApplicationsPETROTHENE LM 6007-00 resin exhibits very low taste and odor characteristics as well as good rigidity. Typical applications include water, and milk and juice bottles.Regulatory StatusLM.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Petrothene® LP5100 High Density Polyethylene ApplicationsPETROTHENE LP 5100 is especially designed for large-part blow molding of durable goods and deep-draw sheet extrusion/thermoforming applications. LP 5100 exhibits excellent impact resist.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Borealis Borstar® HE 6068 Natural Bimodal HDPE with very low shrinkage for Submarine and Fiber Optical Cables Borstar® HE6068 is a natural, UV-stabilized, colorable, bimodal high density (HD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar®.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Borealis HE4872 High Density Polyethylene HE4872 is a HDPE compound for solid insulation of symmetric data cable at high extrusion speed. Applications: high frequency data transmission cables, outer skin of foam-skin constructions. Specif.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Borealis Superclean™ LE4244 Natural Crosslinkable Polyethylene for HIV Power Cable Insulation Superclean LE4244 is a natural crosslinkable polyethylene compound developed especially for the insulation of medium and high voltage cables. It provides an excellent balance of anon-staining antio.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Borealis Visico™/Ambicat™ LE4421/LE4472 Polyethylene Compound, Crosslinkable Visico™ LE4421 / Ambicat™ LE4472 is a silane crosslinkable black compound designed for covering/insulation of overhead cables. The base material Visico™ LE4421 in combination with the catalyst m.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Borealis SuperTR™ LE4212 Scorch Retardant, Crosslinkable Polyethylene, Water Tree Retardant Insulation for Me Power Cables SuperTR LE4212 is a natural, crosslinkable low density polyethylene compound, which has water tree retardant and scorch retardant properties.SuperTR LE4212 has been specifically developed as a scorc.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Dow Engage® 8150 Polyolefin Elastomer Description: Engage® 8150 and Engage® 8157 polyolefin elastomers are ethylene-octene copolymers that have excellent flow characteristics and provide good impact properties in blends with polypropy.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Dow Engage® 8200 Polyolefin Elastomer Description: Engage® 8200 and Engage® 8207 polyolefin elastomers are ethylene-octene copolymers that have excellent flow characteristics and performs well in a wide range of general purpose thermo.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D-746 |
Bapolene® 1072 Polyethylene, Injection Grade A high flow general purpose injection molding resin with good gloss, toughness and stress crack resistance. This product meets FDA standards for food contact applications.Applications: Housewares, .. |
|||
Brittleness Temperature | -76.0 - -42.0 °C | -105 - -43.6 °F | Average value: -70.4 °C Grade Count:10 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Extrusion Grade". Each property range of values reported is min.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Westlake EMAC® SP 1257 Ethylene-Methyl Acrylate Copolymer
(discontinued **) 20% Methyl Acrylate Content. Characteristics: FDA Clearance for Packaging of Most Foods, Including Aseptic Packaging; Less Crystalline and Softer than Polyethylene; Excellent Heat Stability Allows .. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
ExxonMobil Escorene® LD-728 High EVA Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Applications: Injection molding; Foams.. |