| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
|
Network Polymers NPP 50-0350
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
|
|||
| Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
|
Network Polymers NPP 50-1060
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
|
|||
| Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746A |
|
Solvay Specialty Polymers Halar® 500LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)&
Information provided by Solvay Specialty Polymers.
|
|||
| Brittleness Temperature | <= -76.0 °C | <= -105 °F | |
|
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer
(discontinued **)
Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing..
|
|||
| Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
|
LyondellBasell Alathon® L4904 High Density Polyethylene, Pipe and Sheet Extrusion Grade
Alathon L4904 is a bimodal, high molecular weight, high density polyethylene resin with excellent processability characteristics that meet the high performance requirements of demanding pressure pip..
|
|||
| Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
|
LyondellBasell Alathon® M4612 High Density Polyethylene
ApplicationsALATHON M 4612 is a copolymer that provides outstanding ESCR and low temperature impact strength. Typical applications include food containers, seat hinges, tube headers.Regulatory Stat..
|
|||
| Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
|
LyondellBasell Alathon® M4621 High Density Polyethylene
ApplicationsALATHON M 4621 is a copolymer that provides outstanding stress crack resistance and low temperature impact strength. Typical applications include small two-piece engine gas tanks, waste..
|
|||
| Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
|
LyondellBasell Alathon® M5372 High Density Polyethylene
ApplicationsALATHON M 5372 copolymer with narrow weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processing stability. ..
|
|||
| Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
|
LyondellBasell Alathon® M6138 High Density Polyethylene
ApplicationsALATHON M 6138, formerly known as XM 6138, is a high density polyethylene resin for use in injection molding applications. This resin exhibits good impact resistance and high stiffness...
|
|||
| Brittleness Temperature | -76.0 °C | -105 °F | ASTM D746 |
|
LyondellBasell Microthene® F FE53200 Ethylene Vinyl Acetate Copolymer
General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene..
|
|||
| Brittleness Temperature | -76.0 °C | -105 °F | ASTM D746 |
|
LyondellBasell Microthene® F FN51000 Low Density Polyethylene
General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene..
|
|||
| Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
|
LyondellBasell Petrothene® GA808091 Linear Low Density Polyethylene
ApplicationsPETROTHENE GA 808-091 is a broad molecular weight, linear low density polyethylene resin designed for use as a base resin in wire and cable jacketing. An antioxidant package is added to..
|
|||
| Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D2240 |
|
LyondellBasell Petrothene® GA837091 Linear Medium Density Polyethylene
ApplicationsPETROTHENE GA 837-091 is a broad molecular weight, medium density resin designed for extrusion and injection-blow molding. An antioxidant had been added to ensure thermal stability. Pro..
|
|||
| Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
|
LyondellBasell Petrothene® LP500210 High Density Polyethylene (Sheet & Profile Grade)
ApplicationsThe PETROTHENE LP 5002 series of polyethylene resins exhibits excellent environmental stress crack resistance.Regulatory StatusThe LP 5002 base resin meets the requirements of Food and D..
|
|||
| Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
|
LyondellBasell Petrothene® LR732011 High Density Polyethylene (Blow Molding Grade)
ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Typical applications include bottles for bleac..
|
|||
| Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
|
LyondellBasell Petrothene® LR734011 High Density Polyethylene (Sheet & Profile Extrusion)
ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73..
|
|||
| Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
|
LyondellBasell Petrothene® LB500301 High Density Polyethylene, Blow Molding Grade
PETROTHENE LB500301 is a polyethylene resin that exhibits excellent environmental stress crack resistance and is especially designed for heavy duty bottles, such as those containing detergent and ch..
|
|||
| Brittleness Temperature | <= -76.0 °C | <= -105 °F | Procedure A; ASTM D746 |
|
Solvay Specialty Polymers Halar® 350LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol..
|
|||
| Brittleness Temperature | <= -76.0 °C | <= -105 °F | Procedure A; ASTM D746 |
|
Solvay Specialty Polymers Halar® 513LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Low ViscosityUses: MonofilamentsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solv..
|
|||
| Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
|
Borealis Borcell™ HE1102 High Density Polyethylene Compound for Gas Injection of Cellular Communication Cable Insulation
Borcell HE1102 is a high density polyethylene. A nucleating agent is incorporated for a uniform and closed cell structure. The components in the formulation are selected to give the lowest possibl..
|
|||
| Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
|
Borealis HE3366 High Density Polyethylene
HE3366 is a HDPE compound for solid insulation of telephone singles with high extrusion speed. HE3366 is designed as insulation for petroleum filled telephone cables. It is also suitable as outer sk..
|
|||
| Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
|
Borealis Superclean™ LR4201S Crosslinkable Polyethylene Insulation for Medium and High Voltage Power Cables
Superclean LR4201S is a Superclean crosslinkable low density polyethylene (XLPE) for medium and high voltage power cable insulation. The formulation of LR4201S provides an optimum combination of go..
|
|||
| Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
|
ExxonMobil EXACT™ 0230 Plastomer for Multilayer Film Applications
Product Description: Exact 0230 plastomer is an ethylene octene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology. It is designed for both monolayer and multilayer co-extruded cast ..
|
|||
| Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
|
ExxonMobil Paxon™ AB50-003 Blow Molding Resin
Product Description: AB50-003 is a blow molding grade high density polyethylene copolymer. This resin has very good stress crack resistance combined with high impact strength and rigidity.Availabili..
|
|||
| Brittleness Temperature | <= -76.1 °C | <= -105 °F | Molded and tested in accordance with ASTM D4976; ASTM D746 |
|
Dow DNDA-7144 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-7144 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in injection molding applications such as large industrial containers and trash cans. Information provide..
|
|||
| Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
|
Dow Engage® 8207 Polyolefin Elastomer
Description: Engage® 8207 polyolefin elastomer is a loose talc surface coated ethylene-octene copolymer. The talc is untreated and has a nominal 1µm particle size. This product offers the exceptio..
|
|||
| Brittleness Temperature | <= -76.1 °C | <= -105 °F | Molded and tested in accordance with ASTM D4976; ASTM D746 |
|
Dow UNIVAL™ DMDC-6400 NT 7 High Density Polyethylene Resin (HDPE)
Excellent process-ability Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 2.2 UNIVAL™ DMDC-6400 NT 7 is a multipurpose polymer designed for producing containers used to package dairy, wat..
|
|||
| Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
|
ExxonMobil Paxon™ AD60-007 Blow Molding Resin
Product Description: AD60-007 is a medium molecular weight distribution high-density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appear..
|
|||
| Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
|
ExxonMobil Paxon™ BA46-055 Blow Molding Resin
Product Description: BA46-055 is a high molecular weight high density polyethylene copolymer. It possesses a combination of excellent processability, outstanding melt strength, high impact strength..
|
|||
| Brittleness Temperature | <= -76.1 °C | <= -105 °F | ASTM D746 |
|
ExxonMobil Paxon™ AS55-003 Blow Molding Resin
(discontinued **)
AS55-003 is a blow molding grade high density polyethylene copolymer containing an antistat additive. It provides a good balance of stiffness and stress crack resistance.Information provided by Exx..
|
|||