Polymer Property : Density = 0.928 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.928 g/cc
0.0335 lb/in³
ASTM D1505
Chevron Phillips mPact™ D353 m-MDPE Linear Low Density Polyethylene  (discontinued **)
Low Density PolyethyleneCustomer Benefits: This metallocene medium density PE for cast film applications offers greater tensile modulus than LLDPE while retaining excellent optical properties.Data p..
Density 0.928 g/cc
0.0335 lb/in³
Exxon Method
ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Extrusion Coating  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.6.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer designed for extrusion coating, laminating and seaming applications. It can be process..
Density 0.928 - 0.953 g/cc
0.0335 - 0.0344 lb/in³
Average value: 0.940 g/cc Grade Count:22
Overview of materials for EMAAA Terpolymer
This property data is a summary of similar materials in the MatWeb database for the category "EMAAA Terpolymer". Each property range of values reported is minimum and maximum values of appropriate M..
Density 0.928 g/cc
0.0335 lb/in³
ASTM D792
DuPont Appeel® LSR11N704 Lidding Sealant Resin  (discontinued **)
Appeel® 11N704 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide very strong peelable seal..
Density 0.928 - 0.950 g/cc
0.0335 - 0.0343 lb/in³
Average value: 0.938 g/cc Grade Count:30
Overview of materials for Medium Density Polyethylene (MDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim..
Density 0.928 g/cc
0.0335 lb/in³
LyondellBasell Lupolen® 3010 K LDPE, Injection Molding Grade
Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Density 0.928 g/cc
0.0335 lb/in³
LyondellBasell Lupolen® 3020 F LDPE
Blown film, injection moldings, blow moldings.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Density 0.928 g/cc
0.0335 lb/in³
LyondellBasell Lupolen® 3020 H LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Density 0.928 g/cc
0.0335 lb/in³
LyondellBasell Lupolen® 3026 F LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Density 0.928 g/cc
0.0335 lb/in³
LyondellBasell Lupolen® 3032 D LDPE
Insulation for cableData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Density 0.928 - 0.932 g/cc
0.0335 - 0.0337 lb/in³
Kazanorgsintez M 115 Polymer Composition for Rotary Molding
Production Method: Composition is produced on the basis of 11503-070 grade low density polyethylene and 276-03 grade high density polyethylene composition. Application: Compositions are designed..
Density 0.928 - 0.932 g/cc
0.0335 - 0.0337 lb/in³
Kazanorgsintez M 168 Polymer Composition for Rotary Molding
Production Method: Composition is produced on the basis of 11503-070 grade low density polyethylene and 276-03 grade high density polyethylene composition. Application: Compositions are designed..
Density 0.928 g/cc
0.0335 lb/in³
ISO 1183
Borealis Himod™ FT3280 LDPE for Film
Himod FT3280 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
Density 0.928 g/cc
0.0335 lb/in³
ISO 1183
Borealis ME6032 Polypropylene
ME6032 is a MDPE compound for solid insulation of telephone singles and data cables at high line speed. It contains a metal deactivator. Applications: Dry core and petroleum jelly filled cables. S..
Density 0.928 g/cc
0.0335 lb/in³
ASTM D792
DuPont Bynel® 2022 Acid-Modified Ethylene Terpolymer Adhesive Resin
Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature ..
Density 0.928 g/cc
0.0335 lb/in³
ExxonMobil method
ExxonMobil Escorene™ FL 00909 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00909 is used in extrusion coating, cast film and co-extrusion. FL 00909 is good sealing material with good optical properties.Processing Conditions: Excellent results are ob..
Density 0.928 g/cc
0.0335 lb/in³
ExxonMobil method
ExxonMobil LDPE LD 362BR Low Density Polyethylene Resin
Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Density 0.928 g/cc
0.0335 lb/in³
ExxonMobil method
ExxonMobil LDPE LD 362HE Low Density Polyethylene Resin
Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Density 0.928 g/cc
0.0335 lb/in³
ExxonMobil method
ExxonMobil LDPE LD 362ON Low Density Polyethylene Resin
Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Density 0.928 g/cc
0.0335 lb/in³
ExxonMobil method
ExxonMobil LDPE LD 363BR Low Density Polyethylene Resin
Product Description: LD 363 series are LEVA LDPE grades, offering good optical and mechanical properties. Two additive combinations are available according to the required surface properties.Availab..
Density 0.928 g/cc
0.0335 lb/in³
ExxonMobil method
ExxonMobil LDPE LD 364HE Low Density Polyethylene Resin
Product Description: LD 364HE is an LDPE, offering a good combination of mechanical, optical and sealing properties.Availability: Africa & Middle East and Europe Additive: Antiblock: 1500 ppmSlip: ..
Density 0.928 g/cc
0.0335 lb/in³
ExxonMobil method
ExxonMobil Nexxstar™ NX-00328 Low Density Polyethylene Resin
Product Description: Nexxstar 00328 is an LDPE grade, which offers good film rigidity combined with very good optical properties. Its primary use is for high performance collation shrunk packaging.A..
Density 0.928 g/cc
0.0335 lb/in³
Dow DOWLEX™ 2071 Linear Low Density Polyethylene
DOWLEX® 2071 Polyethylene resin is a linear low density polyethylene resin specifically designed for the manufacture of high strength, thin gauge films for use in applications such as grocery sacks..
Density 0.928 g/cc
0.0335 lb/in³
ASTM D792
Dow DOWLEX™ 2071D Linear Low Density Polyethylene
Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow
Density 0.928 g/cc
0.0335 lb/in³
ISO 1183
Fainplast Compounds Ethylplus 611 LE Polyethylene Cable Compound
Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesExpandable LDPEInformation provided by Fainplast Comp..
Density 0.928 g/cc
0.0335 lb/in³
ASTM D792
Dow AMPLIFY™ VA 400 Ethylene vinyl acetate (EVA)
AMPLIFY™ VA 400 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility, clarity and low temperature sealability. It is easy to process and features functional ..
Density 0.928 g/cc
0.0335 lb/in³
BASF Lucalen® A 3110 M Ethylene/Acrylate Copolymer
Economical composite films together with PE-LD; primers for aluminum/steel composites; coatings for paper board, aluminum and steel (e.g. for pipes used to transport petroleum, gas, etc.)Data was co..
Density 0.928 g/cc
0.0335 lb/in³
BASF Lucalen® A 3120 M Ethylene/Acrylate Copolymer
Suitable in similar manner as Lucalen A 2920 M or also as a material for coating aluminum, steel, paper and cardboard. Also for processing pipes for transporting petroleum, gas, etc.Data was collec..
Density 0.928 g/cc
0.0335 lb/in³
Arkema Group Evatane® 1005 VN 3 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for flexible, very transparent film with high strength, shrinking at low temperature. Examples: curtain stretch, coextrusion, ..