Material Notes:
Mylar® HP film is a high strength, high clarity and low haze polyester film with dimensional stability particularly suitable for use in applications where dimensional stability is a requirement during processing. It is used for a broad range of industrial applications. General Product Info: Mylar® HP film has high strength, low haze, and excellent dimensional stability such as its TD shrinkage - zero percent at 150º C/30 min.Typical Applications: Mylar® HP film is designed for roll leaf and metallized labels applications.Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 110 %
110 %
ASTM D882A
Tensile Modulus 4.36 GPa
632 ksi
ASTM D882A
Film Tensile Strength at Break, MD 200 MPa
29000 psi
ASTM D882A
Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
Melting Point 254 °C
489 °F
Typical Mylar® via DSC
Shrinkage, MD 1.5 %

@Temperature 150 °C,
Time 1800 sec
1.5 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 0.00 %

@Temperature 150 °C,
Time 1800 sec
0.00 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Refractive Index 1.64 - 1.67
1.64 - 1.67
typical of Mylar®
Haze 7.0 %
7.0 %
ASTM D1003